Category: | PUR-Ether/TDI , Polyurethane (Polyether, TDI) |
Manufacturer: | Anderson Development Company |
Trademark: | Andur |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | HawZi4_Andur-2-90AP-Curene-280.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
All properties based on Andur® 2-90AP cured with Curene® 280 |
General Information | |
---|---|
Forms |
|
Processing Method |
|
Hardness | Nominal Value | Test Method | |
---|---|---|---|
Durometer Hardness (Shore A) | 85 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | 22.2 | MPa | ASTM D638 |
Tensile Elongation (Break) | 520 | % | ASTM D638 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ASTM D412 | ||
100% strain | 5.03 | MPa | ASTM D412 |
300% strain | 8.27 | MPa | ASTM D412 |
Tear Strength | |||
-- 1 | 63.0 | kN/m | ASTM D624 |
Cracking | 18 | kN/m | ASTM D470 |
Compression Set | 37 | % | ASTM D395 |
Thermoset | Nominal Value | Unit | |
---|---|---|---|
Pot Life | 13 | min | |
Post Cure Time (23°C) | 72 | hr |
Additional Information |
---|
Prepolymer NCO%: 4.0-4.4Grams Curene® 280 per 100 grams prepolymer: 26.6Rebound, %: 52Stoichiometry: 0.95Prepolymer Temperature, °F: 190-210Curene® 280 Temperature, °F: 158Post Cure Time, 212°F, hours: 16 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Mold Temperature | 107 | °C |
Note Message | |
---|---|
1 . | C mould |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 2103 TFE 10 | RTP Company | PEI | RTP |
THERMOLAST® K TF8FMA (Series: FC/AD1) | KRAIBURG TPE | TPE | THERMOLAST® K |
Celstran® +PP-GF60-04CN15 | Celanese Corporation | PP, Unspecified | Celstran® |
DOMAMID® 6G15 | DOMO Engineering Plastics SPA | Nylon 6 | DOMAMID® |
CYCOLAC™ FR15 resin | SABIC Innovative Plastics | ABS | CYCOLAC™ |