Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.07 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) (220°C/10.0 kg) | 5.0 | g/10 min | ASTM D1238 |
Molding Shrinkage - Flow | 0.40 to 0.70 | % |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Rockwell Hardness (R-Scale) | 105 | ASTM D785 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | 41.4 | MPa | ASTM D638 |
Flexural Modulus | 2070 | MPa | ASTM D790 |
Flexural Strength | 62.1 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (3.18 mm) | 190 | J/m | ASTM D256 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load (1.8 MPa, Unannealed) | 93.3 | °C | ASTM D648 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature - Desiccant Dryer | 70.0 to 80.0 | °C | |
Drying Time - Desiccant Dryer | 3.0 | hr | |
Suggested Max Moisture | 0.10 | % | |
Processing (Melt) Temp | 210 to 238 | °C | |
Mold Temperature | 40.0 to 62.8 | °C | |
Injection Pressure | 68.9 to 96.5 | MPa |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
SEETEC PP T3410 | LG Chem Ltd. | PP Terpolymer | SEETEC PP |
SLOVALEN® PH 49 GF 30 TS | Plastcom | PP, Unspecified | SLOVALEN® |
ECOLEN® HZ40P | HELLENIC PETROLEUM S.A. | PP Homopolymer | ECOLEN® |
Eleme HIU07060 | Eleme Petrochemical Company Ltd | HDPE | Eleme |
Grilamid® L XE 10987 black 9225 | EMS-GRIVORY | Nylon 12 | Grilamid® |