| Category: | TPE , Thermoplastic Elastomer |
| Manufacturer: | SABIC Innovative Plastics Europe |
| Trademark: | ISORENE™ |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | HAGzlp_ISORENE-A4-1001.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
ISORENE A4-1001 is a special compound in a natural opaque color for technical applications. The value listed as Strain at Break, ISO 527, was tested in accordance with ISO 37. The value listed as Stress at Break, ISO 527, was tested in accordance with ISO 37. |
| General Information | |
|---|---|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.18 | g/cm³ | ISO 1183 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Shore Hardness (Shore A) | 43 | ISO 868 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Break) | 3.00 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 400 | % | ISO 527-2 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tear Strength | 8.0 | kN/m | ISO 34-1 |
| Compression Set | ISO 815 | ||
| 23°C, 72 hr | 14 | % | |
| 70°C, 24 hr | 30 | % | |
| 100°C, 24 hr | 70 | % |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Instrumented Dart Impact 1(-30°C) | 19.0 | J | ASTM D3763 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| CLTE - Flow (-30 to 60°C) | 1.0E-4 | cm/cm/°C | ASTM D696 |
| Note Message | |
|---|---|
| 1 . | 2.20 m/sec |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Salflex 613TIC | Salflex Polymers Ltd. | PP Copolymer | Salflex |
| VAMPSTAT N 10G 09 V0 26 MF | Vamp Tech | Nylon 6 | VAMPSTAT |
| NEFTEKHIM PP 1300R (Z30G) | Nizhnekamskneftekhim Inc. | PP Homopolymer | NEFTEKHIM PP |
| BorSafe™ HE3494-LS-H | Borealis AG | HDPE | BorSafe™ |
| Eraclene® BB 82 | Versalis S.p.A. | HDPE | Eraclene® |