Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | Kunststoff-Kontor-Hamburg GmbH |
Trademark: | GERMAMID |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | H8nhiV_GERMAMID-6-GK-30.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
GERMAMID 6 GK 30 is a Polyamide 6 (Nylon 6) material filled with 30% glass bead. It is available in Europe. |
General Information | |
---|---|
Filler / Reinforcement |
|
Forms |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.36 | g/cm³ | ISO 1183 |
Molding Shrinkage | 0.50 to 1.5 | % | ISO 294-4 |
Water Absorption (Saturation, 23°C) | 2.0 | % | ISO 62 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 4500 | MPa | ISO 527-2 |
Tensile Stress (Yield) | 80.0 | MPa | ISO 527-2 |
Tensile Strain (Break) | 7.0 | % | ISO 527-2 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength | 6.0 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength | 30 | kJ/m² | ISO 179/1eU |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (0.45 MPa, Unannealed) | 205 | °C | ISO 75-2/B |
Melting Temperature | 218 | °C | |
Thermal Conductivity | 0.28 | W/m/K | ISO 8302 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Surface Resistivity | 1.0E+12 | ohms | IEC 60093 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
SCHULADUR® A NV12LHI | A. Schulman Inc. | PBT | SCHULADUR® |
AMTOPP BTP23 | Inteplast Group | PP, Unspecified | AMTOPP |
Di-Pak™ R-4525/7 | Hapco Inc. | TP, Unspecified | Di-Pak™ |
Sylvin 8280-95UV Black | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
Sylvin 8773-60D White 1403 | Sylvin Technologies Incorporated | PVC, Rigid | Sylvin |