| Category: | TPU-Polyether , Thermoplastic Polyurethane Elastomer (Polyether) |
| Manufacturer: | BASF Polyurethanes GmbH |
| Trademark: | Elastollan® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | G1DAid_Elastollan-1254-D-U.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Highly transparent thermoplastic Polyether Polyurethane Elastomer with good hydrolysis resistance, low temperature flexibility and resistance to micro-organismus Typical applications Ski boot shells, ski components, Films. |
| General Information | |
|---|---|
| Additive |
|
| Features |
|
| Uses |
|
| Appearance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.17 | g/cm³ | ISO 1183/A |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Shore Hardness (Shore D, 3 sec) | 57 | ISO 7619 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 180 | MPa | ISO 527-2 |
| Abrasion Loss | 30.0 | mm³ | ISO 4649-A |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | DIN 53504 | ||
| 20% Strain | 16.5 | MPa | |
| 100% Strain | 23.0 | MPa | |
| 300% Strain | 35.0 | MPa | |
| Tensile Stress | DIN 53504 | ||
| Yield 1 | 53.0 | MPa | |
| Yield | 60.0 | MPa | |
| Tensile Elongation | DIN 53504 | ||
| Break 2 | 520 | % | |
| Break | 470 | % | |
| Tear Strength 3 | 170 | kN/m | ISO 34-1 |
| Compression Set | ISO 815 | ||
| 23°C, 72 hr | 42 | % | |
| 70°C, 24 hr | 54 | % |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179 | ||
| -30°C | 14 | kJ/m² | |
| 23°C | No Break |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Processing (Melt) Temp | 215 to 240 | °C | |
| Mold Temperature | 20.0 to 70.0 | °C |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Melt Temperature | 200 to 230 | °C |
| Note Message | |
|---|---|
| 1 . | after storage in water at 80°C for 42 days |
| 2 . | after storage in water at 80°C for 42 days |
| 3 . | Method Bb, Angle (Nicked) |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| PrimaFlex® HP 1200-F | Plastic Solutions, Inc. | PP Homopolymer | PrimaFlex® |
| RheTech Thermoplastic Polyolefin FT1004-00 | RheTech, Inc. | Polyolefin, Unspecified | RheTech Thermoplastic Polyolefin |
| StarGRIP GP 30-1000 | STAR Thermoplastic Alloys & Rubbers, Inc. | TPE | StarGRIP |
| NAXELL™ PC110M | MRC Polymers, Inc. | PC | NAXELL™ |
| FRblend® PC-1303 | Colour Image Plastic Compound Sdn. Bhd. (CIPC) | PC | FRblend® |