EZPrene 9575A SHF

Category: TPV , Thermoplastic Vulcanizate
Manufacturer: ENPLAST Americas, a Ravago Group Company
Trademark: EZPrene
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: FknuT4_EZPrene-9575A-SHF.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
75 Shore A TPE (Thermoplastic Vulcanizate). Available in black, natural for injection molding applications with long flow lengths or requires highly cosmetic surface. This soft, easy to color material is non-hygroscopic and offers excellent chemical resistance and physical properties. EZPrene 9500 series materials are polyolefin based and 100% recyclable.
General Information
Features
  • Good UV resistance
  • Recyclable materials
  • Good coloring
  • Good adhesion
  • Ozone resistance
  • Good chemical resistance
  • Fatigue resistance
  • Soft
  • Low or no water absorption
Appearance
  • Black
  • Natural color
Processing Method
  • Extrusion
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 0.930g/cm³ASTM D792
HardnessNominal ValueUnitTest Method
Durometer Hardness ASTM D2240
    Shaw A, 5 seconds, extruded 75ASTM D2240
    Shore A, 5 seconds, injection molding 78ASTM D2240
ElastomersNominal ValueUnitTest Method
Tensile Stress (100% Strain)1.50MPaASTM D412
Tensile Strength (Break)4.60MPaASTM D412
Tensile Elongation (Break)510%ASTM D412
Tear Strength 10.5kN/mASTM D624
Compression Set ASTM D395
    23°C, 22 hr 37%ASTM D395
    125°C, 70 hr 54%ASTM D395
ThermalNominal ValueUnitTest Method
Brittleness Temperature -65.0°CASTM D746
Dynamic Service Temperature 130°C
Additional InformationNominal ValueTest Method
Ozone Resistance ExcellentASTM D1149
InjectionNominal ValueUnit
Drying Temperature 82.2°C
Drying Time 2.0 - 3.0hr
Rear Temperature 191 - 204°C
Middle Temperature 196 - 210°C
Front Temperature 196 - 210°C
Nozzle Temperature 210 - 221°C
Processing (Melt) Temp 199 - 221°C
Mold Temperature 23.9 - 51.7°C
Injection Pressure 5.17 - 8.96MPa
Injection Rate Fast
Screw Speed 50 - 200rpm
Clamp Tonnage 2.8 - 4.8kN/cm²
Cushion 5.08 - 12.7mm
Injection instructions
Holding Time: 5 to 7 Sec.Cooling Time: 30 to 50 Sec.
ExtrusionNominal ValueUnit
Hopper Temperature 166 - 177°C
Cylinder Zone 1 Temp. 171 - 191°C
Cylinder Zone 2 Temp. 171 - 191°C
Cylinder Zone 3 Temp. 171 - 191°C
Cylinder Zone 4 Temp. 171 - 191°C
Cylinder Zone 5 Temp. 171 - 191°C
Adapter Temperature 191 - 210°C
Melt Temperature 191 - 199°C
Die Temperature 191 - 210°C
Extrusion instructions
Screw: L/D 24:1 minimumCompression Zone: 355 - 390°F (180 - 200°C)Metering Zone: 375 to 410°F (190 to 210°C)Screw Speed: 30 - 80 rpmScreen Pack: 20/40/60
Resin Grade Manufacturer Category Trademark
Toyolac® 930-355 Toray Resin Company MABS Toyolac®
Fainplast PVC ARC 20 Fainplast Compounds S.r.l PVC, Rigid Fainplast PVC
Fainplast PVC GK 75 Fainplast Compounds S.r.l PVC, Unspecified Fainplast PVC
Duron PEI 5001 ProPolymers Inc. PEI Duron
Clyrell RC6049 LyondellBasell Industries PP, Unspecified Clyrell