| Category: | Nylon 6 , Polyamide 6 |
| Manufacturer: | Polykemi AB |
| Trademark: | SCANAMID 6 |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | Fd2M2i_SCANAMID-6-B11-F30.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Glass fibre-reinforced |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Physical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Density | 1.36 | -- | g/cm³ | ISO 1183 |
| Molding Shrinkage | ISO 294-4 | |||
| Across Flow | 0.90 | -- | % | |
| Flow | 0.30 | -- | % |
| Hardness | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Durometer Hardness (Shore D, 15 sec) | 80 | -- | ASTM D2240 |
| Mechanical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Tensile Stress | 160 | 115 | MPa | ISO 527-2 |
| Tensile Strain (Yield) | 3.0 | 5.0 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 8800 | 5600 | MPa | ISO 178 |
| Flexural Stress | 230 | 140 | MPa | ISO 178 |
| Impact | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179 | |||
| -20°C | -- | 7.0 | kJ/m² | |
| 23°C | 10 | 14 | kJ/m² |
| Thermal | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Heat Deflection Temperature 1 | ||||
| 0.45 MPa, Unannealed | 210 | -- | °C | ISO 75-2/B |
| 1.8 MPa, Unannealed | 200 | -- | °C | ISO 75-2/A |
| Vicat Softening Temperature | 215 | -- | °C | ISO 306/B50 |
| Flammability | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Flame Rating (1.60 mm) | HB | -- | UL 94 | |
| Glow Wire Ignition Temperature (2.00 mm) | 650 | -- | °C | IEC 60695-2-13 |
| Note Message | |
|---|---|
| 1 . | 120°C/hr |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Retpol® 7839/4 HS UV2 | PolyPacific Pty. Ltd. | PP, Unspecified | Retpol® |
| Tarnoform® 500 GF6 | Grupa Azoty S.A. | Acetal (POM) Copolymer | Tarnoform® |
| GAPEX® RPP20EA34NA | Ferro Corporation | PP Homopolymer | GAPEX® |
| Rotuba CAP CP801 (16% Plasticizer) | Rotuba Extruders, Inc. | CAP | Rotuba CAP |
| neogol® A80 2 Z005 | API SpA | TPO (POE) | neogol® |