Category: | TPE , Thermoplastic Elastomer |
Manufacturer: | Mitsubishi Chemical Performance Polymers, Inc. |
Trademark: | tefabloc® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | FBNLA5_tefabloc-TP-SD-300-90A.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
tefabloc®TP SD 300 90A is a thermoplastic elastomer (TPE) material,. This product is available in North America or Europe. The processing method is injection molding. tefabloc®The main features of TP SD 300 90A are:
Typical application areas include:
|
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Resin ID (ISO 1043) |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.890 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 25 | g/10 min | ISO 1133 |
Molding Shrinkage | Internal method | ||
Vertical flow direction | 1.0 | % | Internal method |
Flow direction | 1.1 | % | Internal method |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A, 15 sec, Injection Molded) | 90 | ISO 868 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Abrasion | 130 | mm³ | DIN 53516 |
Aging | Nominal Value | Unit | |
---|---|---|---|
Resistance to Aging | 125 | °C |
Thermal | Nominal Value | Unit | |
---|---|---|---|
Service Temperature | -50 - 70 | °C |
Additional Information | Nominal Value | Test Method | |
---|---|---|---|
Color Fastness | ISO 105-A02 | ||
-- 1 | 4/5 | ISO 105-A02 | |
100 hr | 5 | ISO 105-A02 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ISO 37 | ||
20% strain | 5.70 | MPa | ISO 37 |
100% strain | 6.60 | MPa | ISO 37 |
Tensile Stress (Break) | 9.70 | MPa | ISO 37 |
Tensile Elongation (Break) | 610 | % | ISO 37 |
Tear Strength 2 | 54 | kN/m | ISO 34-1 |
Compression Set 3 | ISO 815 | ||
23°C, 22 hr | 36 | % | ISO 815 |
50°C, 22 hr 4 | 43 | % | ISO 815 |
50°C, 22 hr 5 | 58 | % | ISO 815 |
70°C, 22 hr 6 | 46 | % | ISO 815 |
70°C, 22 hr 7 | 60 | % | ISO 815 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Rear Temperature | 160 | °C | |
Middle Temperature | 170 | °C | |
Front Temperature | 180 | °C | |
Injection Rate | Moderate | ||
Screw Compression Ratio | 2.5:1.0 - 3.0:1.0 |
Injection instructions |
---|
Screw Speed: Medium |
Note Message | |
---|---|
1 . | 1000 hr |
2 . | Method B, right-angle specimen (without cut) |
3 . | Type B |
4 . | relaxation 50°C |
5 . | relaxation 23°C |
6 . | relaxation 70°C |
7 . | relaxation 23°C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Ultrathene® UE637000 | LyondellBasell Industries | EVA | Ultrathene® |
Celanex® 2404 MT | Celanese Corporation | PBT | Celanex® |
Daelim Po1y® PP-124M | DAELIM INDUSTRIAL CO., LTD. | PP, Unspecified | Daelim Po1y® |
INTEGRAL™ 625 | The Dow Chemical Company | Polyolefin, Unspecified | INTEGRAL™ |
Polybutene-1 PB 0110M | LyondellBasell Industries | PB | Polybutene-1 |