Osterlene® PPC20-2.7

Category: PP, High Crystal , High Crystallinity Polypropylene
Manufacturer: Osterman & Company
Trademark: Osterlene®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: EyRCP3_OsterlenePPC2027.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
  • PPC20-2.7 is a high crystallinity, high impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for injection molded small and large appliance parts.
  • Features of PPC20-2.7 include fast molding cycle, good processability, high stiffness, good heat aging resistance, high impact resistance and low warpage.
  • Suggested uses include appliances, crates, packaging, consumer applications, industrial applications and tool/tote boxes.
  • Osterlene PPC20-2.7 meets the requirements of the Food and Drug Administration, 21 CFR Section 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations may apply. Contact your Osterman sales representative for more information.
General Information
Features
  • Low warpage
  • Rigidity, high
  • High crystallization
  • Impact copolymer
  • Impact resistance, high
  • Workability, good
  • Fast molding cycle
  • Medium liquidity
  • Compliance of Food Exposure
Uses
  • Packaging
  • Electrical appliances
  • Tools/Parts Box
  • Industrial application
  • Loading box
Agency Ratings
  • FDA 21 CFR 177.1520
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 0.898g/cm³Internal method
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg)20g/10 minASTM D1238
MechanicalNominal ValueUnitTest Method
Tensile Modulus 1320MPaISO 527-2
Tensile Strength
    Yield 124.4MPaASTM D638
    Yield 24.3MPaISO 527-2/50
Tensile Elongation
    Yield 24.4%ASTM D638
    Fracture 3.4%ISO 527-2/5
Flexural Modulus
    -- 31290MPaASTM D790A
    -- 41480MPaASTM D790B
    -- 1250MPaISO 178
ImpactNominal ValueUnitTest Method
Notched Izod Impact
    23°C 140J/mASTM D256A
    -40°C 4.0kJ/m²ISO 180/1A
    -18°C 4.6kJ/m²ISO 180/1A
    23°C 8.4kJ/m²ISO 180/1A
Note Message
1 .51 mm/min
2 .51 mm/min
3 .1.3 mm/min
4 .13 mm/min
Resin Grade Manufacturer Category Trademark
RABALON® PJ5300C Mitsubishi Chemical Performance Polymers, Inc. TPE RABALON®
Sarlink® TPV X10075B Teknor Apex Company TPV Sarlink® TPV
FHR Polypropylene P6C6B-134 Flint Hills Resources, LP PP Impact Copolymer FHR Polypropylene
K-Bin Rigid PVC KBD-5087 K-Bin, Inc. PVC, Unspecified K-Bin Rigid PVC
RTP 399 X 143537 RTP Company PC RTP