Category: PUR, Unspecified , Polyurethane
Manufacturer: RTP Company
Trademark: RTP
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: EsAHAa_RTP-2302-C.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Glass Fiber
General Information
Filler / Reinforcement
  • Glass fiber reinforced material, 15% filler by weight
RoHS Compliance
  • Contact manufacturer
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.29g/cm³ASTM D792
Molding Shrinkage - Flow (3.20 mm)0.20 - 0.40%ASTM D955
Moisture Content 0.010%
Additional InformationNominal ValueUnit
Primary Additive 15%
MechanicalNominal ValueUnitTest Method
Tensile Modulus 4480MPaASTM D638
Tensile Strength 103MPaASTM D638
Tensile Elongation (Yield)4.0 - 6.0%ASTM D638
Flexural Modulus 4480MPaASTM D790
Flexural Strength 152MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (3.20 mm)110J/mASTM D256
Unnotched Izod Impact (3.20 mm)370J/mASTM D4812
FlammabilityNominal ValueTest Method
Flame Rating (1.50 mm, ** Values per RTP Company testing.)HBUL 94
InjectionNominal ValueUnit
Drying Temperature 132°C
Drying Time 4.0 - 6.0hr
Dew Point -40.0°C
Processing (Melt) Temp 238 - 260°C
Mold Temperature 93.3 - 121°C
Injection Pressure 68.9 - 103MPa
Injection instructions
Desiccant Type Dryer Required.
Resin Grade Manufacturer Category Trademark
ALTECH® PA66 A 2040/100.01 GF40 ALBIS PLASTIC GmbH Nylon 66 ALTECH® PA66
GAPEX® FPP30GQ03HB TAN Ferro Corporation PP, Unspecified GAPEX®
HI-ZEX™ 3600F Prime Polymer Co., Ltd. HDPE HI-ZEX™
Karina CLEAR PVC COMPOUND 80/231-P-IS-AS Karina Ind. e Com. de Plásticos Ltda PVC, Unspecified Karina
Sylvin 916VO-85 Brown 7406 Sylvin Technologies Incorporated PVC, Unspecified Sylvin