Monprene®OM-10185 is a thermoplastic elastomer (TPE) material,. This product is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. The processing method is extrusion or injection molding.

Monprene®The main features of the OM-10185 are:
  • ROHS certification
  • Good processability
  • Strong adhesion
  • high hardness
  • Wear-resistant

Typical application areas include:
  • Handle
  • engineering/industrial accessories
  • Electrical/electronic applications
  • electrical appliances
  • Tools
General Information
Features
  • Low Specific Gravity
  • Low density
  • smoothness
  • Light stabilization
  • Workability, good
  • Adhesiveness
  • Good formability
  • Good processing stability
  • Good liquidity
  • Good color stability
  • Good coloring
  • Good wear resistance
  • Medium liquidity
  • Good demoulding performance
  • High hardness
Uses
  • Handle
  • overmolding
  • Electrical appliances
  • Power/other tools
  • Soft handle
  • Mobile phone
  • Sporting goods
  • Stationery
  • Knob
  • Dental application field
  • Toothbrush handle
  • Bonding
RoHS Compliance
  • RoHS compliance
Appearance
  • Opacity
  • Available colors
  • Natural color
Forms
  • Particle
Processing Method
  • Extrusion
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 0.938g/cm³ASTM D792
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg)7.0g/10 minASTM D1238
HardnessNominal ValueUnitTest Method
Durometer Hardness ASTM D2240
    Shore A, 1 second, injection molding 87ASTM D2240
    Shore A, 5 seconds, injection molding 85ASTM D2240
ElastomersNominal ValueUnitTest Method
Tensile Stress 1ASTM D412
    Transverse flow : 100% strain 5.28MPaASTM D412
    Flow : 100% strain 8.31MPaASTM D412
    Transverse flow : 300% strain 6.79MPaASTM D412
Tensile Strength 2ASTM D412
    Transverse flow : Fracture 10.2MPaASTM D412
    Flow : Fracture 10.2MPaASTM D412
Tensile Elongation 3ASTM D412
    Transverse flow : Fracture 560%ASTM D412
    Flow : Fracture 230%ASTM D412
Tear Strength 4ASTM D624
    Transverse flow 63.4kN/mASTM D624
    Flow 54.6kN/mASTM D624
Compression Set 5ASTM D395B
    23°C, 22 hr 22%ASTM D395B
    70°C, 22 hr 94%ASTM D395B
Additional InformationNominal Value
Adhesion to Nylon
Legal statement
The information and recommendations contained in this bulletin are, to the best of our knowledge, accurate and reliable but no guarantee of their accuracy is made. All products are sold upon condition that purchasers shall make their own tests to determine the suitability of such products for their particular purposes and uses and purchaser assumes all risks and liability for the results of use of the products, including use in accordance with seller's recommendations. Nothing in this bulletin constitutes permission or a recommendation to practice or use any invention covered by any patent owned by this company or others. There is no warranty of merchantability and there are no other warranties for the products described. For detailed Product Stewardship information, please contact us. Any product of Teknor Apex, including product names, shall not be used or tested in medical or food contact applications without the prior written acknowledgement of Teknor Apex as to the intended use. Please note that some products may not be available in one or more countries.
InjectionNominal ValueUnit
Drying Temperature 60°C
Drying Time 2.0 - 4.0hr
Rear Temperature 204 - 238°C
Middle Temperature 204 - 238°C
Front Temperature 204 - 238°C
Nozzle Temperature 204 - 238°C
Processing (Melt) Temp 204 - 238°C
Mold Temperature 16 - 32°C
Injection Pressure 1.38 - 5.52MPa
Back Pressure 0.172 - 0.862MPa
Screw Speed 50 - 100rpm
Cushion 3.81 - 25.4mm
Injection instructions
Moisture can degrade the material. Drying is suggested. This can be accomplished by placing the material in a desiccant dryer for 2 to 4 hours at 140°F.
ExtrusionNominal ValueUnit
Cylinder Zone 1 Temp. 193 - 238°C
Cylinder Zone 2 Temp. 193 - 238°C
Cylinder Zone 3 Temp. 193 - 238°C
Cylinder Zone 4 Temp. 193 - 238°C
Cylinder Zone 5 Temp. 193 - 238°C
Die Temperature 193 - 238°C
Note Message
1 .C mold, 510mm/min
2 .C mold, 510mm/min
3 .C mold, 510mm/min
4 .C mold, 510mm/min
5 .Type 1
Resin Grade Manufacturer Category Trademark
PPR PPHO03 Premier Plastic Resins, Inc. PP Homopolymer PPR
PRL NY66-GP1 Polymer Resources Ltd. Nylon 66 PRL
Baoding 68T90 Baoding Bangtai Polymeric New-Materials Co.,Ltd TPU-Polyester Baoding
Hyundai EP TOP COAT PT900W / 2101 HYUNDAI EP Co., Ltd. PP, Unspecified Hyundai EP TOP COAT
Monprene® MP-1500 Teknor Apex Company TPE Monprene®