Category: | PC+ABS , Polycarbonate + ABS |
Manufacturer: | A. Schulman Europe |
Trademark: | SCHULABLEND® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | EMoHwg_SCHULABLENDMMB5301.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
PC/ABS Alloy |
General Information | |
---|---|
Features |
|
Uses |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.12 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (260°C/5.0 kg) | 20 | g/10 min | ISO 1133 |
Molding Shrinkage | 0.50 - 0.70 | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 2350 | MPa | ISO 527-2 |
Tensile Stress (Yield) | 53.0 | MPa | ISO 527-2 |
Tensile Strain (Break) | > 50 | % | ISO 527-2 |
Flexural Modulus | 2200 | MPa | ISO 178 |
Flexural Stress | 75.0 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (23°C) | 40.0 | kJ/m² | ASTM D256 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature | |||
0.45 MPa, not annealed | 123 | °C | ISO 75-2/B |
1.8 MPa, not annealed | 100 | °C | ISO 75-2/A |
Vicat Softening Temperature | 120 | °C | ISO 306/B50 |
Flammability | Nominal Value | Test Method | |
---|---|---|---|
Flame Rating | HB | UL 94 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 100 | °C | |
Drying Time | 4.0 | hr | |
Suggested Max Moisture | 0.020 | % | |
Suggested Max Regrind | 20 | % | |
Processing (Melt) Temp | 260 - 280 | °C | |
Mold Temperature | 70 - 100 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
TAROMID B 280 G6 | Taro Plast S.p.A. | Nylon 6 | TAROMID B |
THERMOLAST® K TC5TPZ (Series: GP/AP) | KRAIBURG TPE | TPE | THERMOLAST® K |
Nylene® 323 | Custom Resins Group | Nylon 6 | Nylene® |
Hostacom TRC 333N D72643 | LyondellBasell Industries | PP Copolymer | Hostacom |
Politen® G2FR05 | ITEN INDUSTRIES | Polyester Alloy | Politen® |