Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | Solvay Engineering Plastics |
Trademark: | TECHNYL® C |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | DbrXrg_TECHNYL-C-52G1-V25-GREY-R7035-CF.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Polyamide 6, Glass-filled, glow-wire modified, color stabilised, lubricated for injection moulding. |
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Uses |
|
Appearance |
|
Processing Method |
|
Part Marking Code (ISO 11469) |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.35 | -- | g/cm³ | ISO 1183/A |
Molding Shrinkage | Internal Method | |||
Across Flow | 0.85 | -- | % | |
Flow | 0.65 | -- | % | |
Water Absorption (23°C, 24 hr) | 1.1 | -- | % | ISO 62 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus | 6850 | 4350 | MPa | ISO 527-2/1A |
Tensile Stress (Break) | 85.0 | 51.0 | MPa | ISO 527-2/1A |
Tensile Strain (Break) | 2.7 | 4.2 | % | ISO 527-2/1A |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength | 3.5 | 8.6 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength | 41 | 84 | kJ/m² | ISO 179/1eU |
Notched Izod Impact Strength | 4.7 | -- | kJ/m² | ISO 180/1A |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 1.70 | -- | °C | ISO 75-2/Af |
Melting Temperature | 220 | -- | °C | ISO 11357-3 |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Comparative Tracking Index (Solution A) | 550 | -- | V | IEC 60112 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Flame Rating | UL 94 | |||
0.800 mm | V-2 | -- | ||
1.60 mm | V-2 | -- | ||
Glow Wire Flammability Index | IEC 60695-2-12 | |||
0.800 mm | 960 | -- | °C | |
1.60 mm | 960 | -- | °C |
Injection | Dry | Unit | |
---|---|---|---|
Drying Temperature | 80.0 | °C | |
Suggested Max Moisture | 0.20 | % | |
Rear Temperature | 230 to 240 | °C | |
Middle Temperature | 235 to 245 | °C | |
Front Temperature | 240 to 250 | °C | |
Mold Temperature | 60.0 to 90.0 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
PRL NY66-GP2-(color)H | Polymer Resources Ltd. | Nylon 66 | PRL |
Addisil™ 8101 | Momentive Performance Materials Inc. | Silicone | Addisil™ |
Axiall PVC 8491 | Axiall Corporation | PVC, Semi-Rigid | Axiall PVC |
Gebalon 15-141 HI | geba Kunststoffcompounds GmbH | PC | Gebalon |
LubriOne™ PC-20GF/15T NC042 S-RoHs | PolyOne Corporation | PC | LubriOne™ |