| Category: | PE, Unspecified , Polyethylene |
| Manufacturer: | Ensinger GmbH |
| Trademark: | TECACOMP® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | DSB0Gb_TECACOMPPEIDblue3943.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
Main features
|
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Features |
|
| Agency Ratings |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.26 | g/cm³ | |
| Melt Mass-Flow Rate (MFR) (230°C/5.0 kg) | 19 | g/10 min | ISO 1133 |
| Melt Volume-Flow Rate (MVR) (230°C/5.0 kg) | 18.0 | cm³/10min | ISO 1133 |
| Molding Shrinkage | ISO 294-4 | ||
| Transverse flow | 1.8 | % | ISO 294-4 |
| Flow | 3.0 | % | ISO 294-4 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 170 | MPa | ISO 527-2/50 |
| Tensile Stress | 10.0 | MPa | ISO 527-2/50 |
| Tensile Strain (Break) | 110 | % | ISO 527-2/50 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Unnotched Impact Strength | No Break | ISO 179/1eU |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Melting Temperature | 130 - 145 | °C | DIN 53765 |
| Service Temperature | |||
| long term | 70 | °C | |
| short term | 100 | °C |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 80 | °C | |
| Drying Time | 2.0 - 4.0 | hr | |
| Suggested Max Moisture | 0.10 | % | |
| Processing (Melt) Temp | 200 - 260 | °C | |
| Mold Temperature | 40 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| NuSil CV-2187 | NuSil Technology | Silicone | NuSil |
| Bayblend® FR3005 BBS310 | Covestro - Polycarbonates | PC+ABS | Bayblend® |
| BESTNYL SI15VI02BX | Triesa Plastics | Nylon 6 | BESTNYL |
| Drystar™ 0831 | Eastman Chemical Company | Copolyester | Drystar™ |
| HAIPLEN H30 G8 BA | Taro Plast S.p.A. | PP Homopolymer | HAIPLEN |