| Category: | EVA , Ethylene Vinyl Acetate Copolymer Resin |
| Manufacturer: | ExxonMobil Chemical |
| Trademark: | Escorene™ Ultra |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | DKs82m_Escorene-Ultra-FL-00226CC.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| FL 00226CC is a copolymer of ethylene and vinyl acetate with low crystal point. When the processing temperature is higher than 230 C (446 °F) in processing conditions, resin degradation may be caused. The machine should be thoroughly cleaned with low density polyethylene or suitable detergent before stopping. |
| General Information | |
|---|---|
| Additive |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Vinyl Acetate Content | 26.0 | wt% | ExxonMobil Method |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A, 15 sec) | 82 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus 1 | 20.0 | MPa | ASTM D638 |
| Tensile Elongation 2(Break) | > 100 | % | ASTM D638 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Vicat Softening Temperature | 47.0 | °C | ASTM D1525 |
| Legal statement |
|---|
| 有关潜在食品接触应用合规信息(例如:FDA、EU、HPFB),请与埃克森美孚化工客户服务代表联系。本产品不宜在医疗应用中使用,亦不应在任何此类应用中使用 |
| Note Message | |
|---|---|
| 1 . | 5.0 mm/min |
| 2 . | 500 mm/min |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 802 GB 20 | RTP Company | Acetal (POM) Copolymer | RTP |
| Terblend® N NM-19XP | INEOS Styrolution Group GmbH | ABS+Nylon | Terblend® N |
| KOCETAL® K300EW | Kolon Plastics, Inc. | Acetal (POM) Copolymer | KOCETAL® |
| Hostacom ERC 161N | LyondellBasell Industries | PP Copolymer | Hostacom |
| Optix® CA-927 | Plaskolite West, Inc. | Acrylic (PMMA) | Optix® |