Miramid® VE50C is a Polyamide 6 (Nylon 6) material filled with 50% glass fiber. It is available in Europe for injection molding. Important attributes of Miramid® VE50C are:
Typical applications include:
|
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Uses |
|
Forms |
|
Processing Method |
|
Multi-Point Data |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1560 | -- | kg/m³ | ISO 1183 1 |
Water Absorption | ISO 62 2 | |||
Saturation | 4.8 | -- | % | |
Equilibrium | 1.2 | -- | % | |
Viscosity number | 140 | -- | cm³/g | ISO 307, 1157, 1628 3 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile modulus | 15500 | 10500 | MPa | ISO 527-2 4 |
Tensile Stress (Break) | 210 | 150 | MPa | ISO 527-2 5 |
Tensile Strain (Break) | 2.5 | 4.0 | % | ISO 527-2 6 |
Flexural Stress 7 | 320 | 230 | MPa | ISO 178 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy notched impact strength | ISO 179/1eA 8 | |||
-30°C | 13.0 | -- | kJ/m² | |
23°C | 15.0 | 17.0 | kJ/m² | |
Charpy impact strength | ISO 179/1eU 9 | |||
-30°C | 75.0 | -- | kJ/m² | |
23°C | 95.0 | 105 | kJ/m² |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Deflection Temperature Under Load | ISO 75-2 10 | |||
0.45 MPa | 215 | -- | °C | |
1.8 MPa | 210 | -- | °C | |
Melting Temperature (DSC) | 220 | -- | °C | ISO 3146 |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Volume resistivity | 1.0E+13 | 1.0E+10 | ohms·m | IEC 60093 11 |
Dielectric Constant (1 MHz) | 3.90 | 6.00 | IEC 60250 | |
Dissipation Factor (1 MHz) | 0.015 | 0.15 | IEC 60250 12 | |
Comparative tracking index | 550 | -- | IEC 60112 13 |
Injection | Dry | Unit | |
---|---|---|---|
Processing (Melt) Temp | 260 to 290 | °C | |
Mold Temperature | 80.0 to 120 | °C |
Note Message | |
---|---|
1 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
2 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
3 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
4 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
5 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
6 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
7 . | Typical values for uncoloured product at 23°C |
8 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
9 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
10 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
11 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
12 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
13 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
VAMPSTAT N 10G 09 V0 26 MF | Vamp Tech | Nylon 6 | VAMPSTAT |
CERTENE™ LLHC-217A | Muehlstein | LLDPE | CERTENE™ |
Chemlon® 143 G | Teknor Apex Company (Chem Polymer) | Nylon 66 | Chemlon® |
Lupoy® EU5008 | LG Chem Ltd. | ASA+PC | Lupoy® |
Styroflex® 2G66 | INEOS Styrolution Group GmbH | SBC | Styroflex® |