Carbon Fiber
General Information
Filler / Reinforcement
  • Carbon fiber reinforced material, 30% filler by weight
RoHS Compliance
  • Contact manufacturer
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.50g/cm³ASTM D792
Molding Shrinkage - Flow (3.20 mm)0.050 - 0.10%ASTM D955
MechanicalNominal ValueUnitTest Method
Tensile Modulus 27600MPaASTM D638
Tensile Strength 200MPaASTM D638
Tensile Elongation (Yield)2.0%ASTM D638
Flexural Modulus 24100MPaASTM D790
Flexural Strength 290MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (3.20 mm)110J/mASTM D256
Unnotched Izod Impact (3.20 mm)480J/mASTM D4812
ThermalNominal ValueUnitTest Method
Deflection Temperature Under Load (1.8 MPa, Unannealed)229°CASTM D648
Additional InformationNominal ValueUnit
Primary Additive 30%
InjectionNominal ValueUnit
Drying Temperature 149°C
Drying Time 4.0hr
Processing (Melt) Temp 271 - 302°C
Mold Temperature 37.8 - 93.3°C
Injection Pressure 34.5 - 82.7MPa
Injection instructions
The key to successfully molding this material is to start mold open cycles as soon as the screw reaches its retracted position.
Resin Grade Manufacturer Category Trademark
RTP 205 SI 2 Z RTP Company Nylon 66 RTP
SLOVALEN® PH 56 FRD 1 Plastcom PP, Unspecified SLOVALEN®
Ferro PP MPP20FJ12BK Ferro Corporation PP Homopolymer Ferro PP
Osterlene® PPH20 Osterman & Company PP Homopolymer Osterlene®
Sylvin 9928-80 Black Sylvin Technologies Incorporated PVC, Unspecified Sylvin