EverGlide® 1908

Category: Nylon 6 , Polyamide 6
Manufacturer: Polymer Dynamix
Trademark: EverGlide®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: CKBe8I_EverGlide-1908.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
EverGlide™ 1908 is reactively modified nylon 6 resin designed for extrusion and injection molding applications. The EverGlide™ 1908 resin is highly lubricious and abrasion resistant and does not make use of additives or particulate modifiers which may be prone to being wiped off the surface, or pulled out of the resin. The unique chemistry and modification in the EverGlide™ 1908 allows for a material that has a surface that will self-heal in cases of extreme abrasion, marring or scratches.

Features:
  • Fast Cycling
  • Lower Surface COF
  • Best in class Mar and Abrasion Resistance
  • Increased Hydrophobicity
  • Self Healing surface parts appear defect free
  • Print and paintability similar to PA 6
  • Good ahesion to PVC

Applications:
  • Films
  • Automotives
  • Wire and Cable (easy to install wire)
  • Electronics
  • Housings
  • Packaging
  • Military
General Information
Features
  • Sprayable
  • Good wear resistance
  • Good adhesion
  • Self-repair
Uses
  • Films
  • Electrical/Electronic Applications
  • Military application
  • Application in Automobile Field
Agency Ratings
  • FDA not rated
Processing Method
  • Extrusion
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.10g/cm³ASTM D792
MechanicalNominal ValueUnitTest Method
Tensile Strength ASTM D638
    Yield 51.0MPaASTM D638
    Fracture 37.9MPaASTM D638
Tensile Elongation ASTM D638
    Yield 8.0%ASTM D638
    Fracture 40 - 50%ASTM D638
Flexural Modulus 1520MPaASTM D790
Flexural Strength 56.5MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (23°C, 3.18 mm)64J/mASTM D256
InjectionNominal ValueUnit
Drying Temperature 82.2 - 87.8°C
Drying Time 2.0 - 4.0hr
Suggested Max Moisture 0.12%
Rear Temperature 232 - 260°C
Middle Temperature 238 - 266°C
Front Temperature 243 - 271°C
Nozzle Temperature 249 - 277°C
Processing (Melt) Temp 249 - 277°C
Mold Temperature 65.6 - 93.3°C
Injection Pressure 34.5 - 138MPa
Injection Rate Moderate
Screw Speed 40 - 70rpm
Clamp Tonnage 4.1 - 6.9kN/cm²
ExtrusionNominal ValueUnit
Drying Temperature 82.2 - 87.8°C
Drying Time 2.0 - 4.0hr
Cylinder Zone 1 Temp. 232 - 260°C
Cylinder Zone 3 Temp. 238 - 266°C
Cylinder Zone 5 Temp. 243 - 271°C
Melt Temperature 249 - 277°C
Die Temperature 249 - 277°C
Extrusion instructions
Suggested Max Moisture: .12%
Resin Grade Manufacturer Category Trademark
Premi-Ject® 6100-10 Premix, Inc. TS, Unspecified Premi-Ject®
Sarlink® TPV X5745B Teknor Apex Company TPV Sarlink® TPV
Monprene® IN-22058 XRD (PRELIMINARY DATA) Teknor Apex Company TPE Monprene®
Nylene® 4114-14 Custom Resins Group Nylon 66 Nylene®
Huafon JF-HSY-9510 Huafon Group Co., Ltd. PUR, Unspecified Huafon