Hanwha CHNA-8380 is a high molecular weight, high density polyethylene(HDPE) insulation compound especially designed for high-speed wire insulating extrusion process. It provides excellent processability, environmental and thermal stress cracking resistance. It meets major international aging test specification for both solid and foam/skin insulation. It can be used for the full range of telephone cable insulation including air-core, jelly-filled and LAN cable (Cat. 5/5e).
General Information
Features
  • Good Processability
  • High Density
  • High ESCR (Stress Crack Resist.)
  • High Molecular Weight
Uses
  • Communication Wire Insulation
  • Wire & Cable Applications
Agency Ratings
  • ASTM D 1248, III, Class A, Cat. 4, Grade E8
  • ASTM D 1248, III, Class A, Cat. 4, Grade E9
  • BS 6234 Type H03
  • ICEA S-84-608
  • IEC 60708
  • NF C 32-060
Forms
  • Pellets
Processing Method
  • Extrusion
  • Wire & Cable Extrusion
PhysicalNominal ValueUnitTest Method
Density 0.945g/cm³ASTM D1505
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg)0.70g/10 minASTM D1238
Environmental Stress-Cracking Resistance (50°C, 10% Igepal, F0)> 1000hrASTM D1693
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shore D, 1 sec)53ASTM D2240
MechanicalNominal ValueUnitTest Method
Tensile Strength 23.5MPaASTM D638
Tensile Elongation (Break)550%ASTM D638
AgingNominal ValueUnitTest Method
Oven Aging (100°C)2.0day
Retention of Tensile Elongation - 2 days (100°C)> 90%ASTM D638
Retention of Tensile Strength - 2 days (100°C)> 90%ASTM D638
ThermalNominal ValueUnitTest Method
Oxidation Induction Time - AI (200°C)> 100minASTM D3895
Thermal Stress Crack Resistance > 96hrASTM D2951
Brittleness Temperature < -76.0°CASTM D746
ElectricalNominal ValueUnitTest Method
Volume Resistivity > 1.0E+16ohms·cmASTM D257
Dielectric Constant (1 MHz)< 2.30ASTM D150
Dissipation Factor (1 MHz)< 1.0E-4ASTM D150
ExtrusionNominal ValueUnit
Melt Temperature 240 to 280°C
Resin Grade Manufacturer Category Trademark
Stanyl® ForTii™ TX1 DSM Engineering Plastics Nylon 4T Stanyl® ForTii™
ALTECH® PA6 A 1000/126 UV ALBIS PLASTIC GmbH Nylon 6 ALTECH® PA6
Clariant Nylon 6/6 PA-133G13 Clariant Corporation Nylon 66 Clariant Nylon 6/6
Hifax TSOP EM7 BLACK LyondellBasell Industries Polyolefin, Unspecified Hifax
ESTOPLAST EP 2015BB01 Ester Industries Ltd. PBT ESTOPLAST EP