Category: | TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester) |
Manufacturer: | Covestro - PUR |
Trademark: | Desmopan® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | BnGze1_Desmopan-DP-3378A.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Extrusion grade; Hoses, non-reinforced |
General Information | |
---|---|
Uses |
|
RoHS Compliance |
|
Processing Method |
|
Hardness | Nominal Value | Test Method | |
---|---|---|---|
Shore Hardness (Shore A) | 80 | ISO 868 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress 1 | DIN 53504 | ||
Break, 23°C | 43.0 | MPa | |
100% Strain, 23°C | 3.90 | MPa | |
300% Strain, 23°C | 9.70 | MPa | |
Tensile Strain 2(Break, 23°C) | 680 | % | DIN 53504 |
Abrasion Resistance (23°C) | 31.0 | mm³ | ISO 4649-A |
Tensile Storage Modulus | ISO 6721-1,-4 | ||
-20°C | 46.0 | MPa | |
20°C | 22.0 | MPa | |
60°C | 12.0 | MPa |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Impact Resilience (23°C) | 57 | % | ISO 4662 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tear Strength 3(23°C) | 67 | kN/m | ISO 34-1 |
Compression Set | ISO 815 | ||
23°C, 72 hr | 46 | % | |
70°C, 24 hr | 19 | % |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | < 90.0 | °C | |
Processing (Melt) Temp | 210 to 230 | °C | |
Mold Temperature | 20.0 to 40.0 | °C |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | < 90.0 | °C | |
Melt Temperature | 200 to 220 | °C |
Note Message | |
---|---|
1 . | 200 mm/min |
2 . | 200 mm/min |
3 . | 500 mm/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 2800B-50D HF | RTP Company | TPV | RTP |
TRIEL® 5722EM | Samyang Corporation | TPEE | TRIEL® |
Badamid® LB70 GF30 | Bada AG | Nylon 6 | Badamid® |
Evoprene™ GC 5615 | AlphaGary | SEBS | Evoprene™ GC |
Lionpol IM-40077 | Lion Polymers Incorporated | TPE | Lionpol |