Category: | TPV , Thermoplastic Vulcanizate |
Manufacturer: | Riken Technos Corp. |
Trademark: | Supersoft Actymer® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | BGdfNc_Supersoft-Actymer-AE-2000S.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Supersoft Actymer®AE-2000S is a thermoplastic vulcanized rubber (TPV) product,. It is available in North America or Asia Pacific. |
General Information | |
---|---|
Features |
|
Forms |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.918 | g/cm³ | ISO 1183 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A, 15 sec) | 3 | ISO 868 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (100% Strain) | 0.100 | MPa | ISO 37 |
Tensile Stress (Yield) | 1.70 | MPa | ISO 37 |
Tensile Elongation (Break) | 830 | % | ISO 37 |
Tear Strength | 8.0 | kN/m | ISO 34-1 |
Compression Set | ISO 815 | ||
70°C, 72 hr | 28 | % | ISO 815 |
120°C, 72 hr | 64 | % | ISO 815 |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Tensile Strength in Air (136°C, 168 hr) | -10 | % | ISO 188 |
Change in Tensile Strain at Break in Air (136°C, 168 hr) | -20 | % | ISO 188 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Brittleness Temperature | -60.0 | °C | ISO 974 |
Additional Information |
---|
The values listed above are tested in accordance with JIS K test methods.Rebound Resilience: 40% |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Sunny® PA6 EB230 | Guangdong Shunde Shunyan New Material Co., Ltd. | Nylon 6 | Sunny® |
Celstran® PP-GF30-0405 P10/16 | Celanese Corporation | PP, Unspecified | Celstran® |
Lucent PC PC/PBT-1420IM | Lucent Polymers, Inc. | PC+PBT | Lucent PC |
Daelim Po1y® XP9500 | DAELIM INDUSTRIAL CO., LTD. | mLLDPE | Daelim Po1y® |
Novalloy-S S5230 | PlastxWorld Inc. | PC+ABS | Novalloy-S |