RTP 200 TFE 30

Category: Nylon 66 , Polyamide 66
Manufacturer: RTP Company
Trademark: RTP
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: B7NFvl_RTP-200-TFE-30.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
PTFE Lubricated
General Information
Additive
  • PTFE lubricant (30%)
Features
  • Lubrication
RoHS Compliance
  • Contact manufacturer
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.33g/cm³ASTM D792
Molding Shrinkage - Flow (3.20 mm)1.5 - 2.5%ASTM D955
Moisture Content 0.20%
Additional InformationNominal ValueUnit
Primary Additive 30%
MechanicalNominal ValueUnitTest Method
Tensile Modulus 2620MPaASTM D638
Tensile Strength 58.6MPaASTM D638
Tensile Elongation (Yield)> 7.0%ASTM D638
Flexural Modulus 2480MPaASTM D790
Flexural Strength 86.2MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (3.20 mm)59J/mASTM D256
Unnotched Izod Impact (3.20 mm)480J/mASTM D4812
ThermalNominal ValueUnitTest Method
Deflection Temperature Under Load (1.8 MPa, Unannealed)82.2°CASTM D648
ElectricalNominal ValueUnitTest Method
Volume Resistivity > 1.0E+14ohms·cmASTM D257
FlammabilityNominal ValueUnitTest Method
Flame Rating (1.50 mm, ** Values per RTP Company testing.)HBUL 94
InjectionNominal ValueUnit
Drying Temperature 79.4°C
Drying Time 4.0hr
Dew Point -17.8°C
Processing (Melt) Temp 277 - 299°C
Mold Temperature 65.6 - 107°C
Injection Pressure 68.9 - 124MPa
Injection instructions
Desiccant Type Dryer Required.
Resin Grade Manufacturer Category Trademark
RxLOY™ FFS-NPP00NP01NA Ferro Corporation PP Alloy RxLOY™
Rotec® ASA S 510 ROMIRA GmbH ASA Rotec® ASA
Elastron® TPO T401.D51.N Elastron USA, Inc. TPO (POE) Elastron® TPO
LAMIGAMID® 310 Schwartz Technical Plastic Nylon 6 LAMIGAMID®
Sylvin 8036-65 Clear 876 Sylvin Technologies Incorporated PVC, Unspecified Sylvin