| Category: | HDPE , High Density Polyethylene |
| Manufacturer: | HP-T Höglmeier Polymer-Tech GmbH & Co. KG |
| Trademark: | Hoegolup® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | AYDpDg_Hoegolup-AIM-blue-5117.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
Product features:
Applications:
|
| General Information | |
|---|---|
| Additive |
|
| Features |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density (23°C) | 0.945 | g/cm³ | DIN 53479 |
| Melt Mass-Flow Rate (MFR) (190°C/21.6 kg) | 15 | g/10 min | ISO 1133 |
| Melt Volume-Flow Rate (MVR) (190°C/21.6 kg) | 19.0 | cm³/10min | ISO 1133 |
| Ash Content | < 0.10 | % | DIN EN 60 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Shore Hardness (Shore D) | 62 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 818 | MPa | ISO 527-2 |
| Tensile Stress | ISO 527-2 | ||
| Break | 15.0 | MPa | |
| -- | 21.0 | MPa | |
| Tensile Strain (Break) | > 100 | % | ISO 527-2 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Peak Crystallization Temperature (DSC) | 130 | °C | ISO 3146 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Processing (Melt) Temp | 250 to 280 | °C | |
| Mold Temperature | 30.0 to 60.0 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 200 GB 13 | RTP Company | Nylon 66 | RTP |
| Viton® VTR-8530 | DuPont Performance Elastomers | Fluorelastomer | Viton® |
| KOPLA PET KEG1030F | KOPLA Co., Ltd. | PET | KOPLA PET |
| StarPrene® 6203-50D | Star Thermoplastic Alloys & Rubbers, Inc. | TPE | StarPrene® |
| Sylvin 9077-90 Brown 7141 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |