Grilamid® L 25 W 10 H X is a Polyamide 12 (Nylon 12) material. It is available in Africa & Middle East, Asia Pacific, Europe, Latin America, or North America for extrusion.

Important attributes of Grilamid® L 25 W 10 H X are:
  • Flame Rated
  • RoHS Compliant
  • Plasticized
  • Good Flexibility
  • Heat Stabilizer

Typical applications include:
  • Automotive
  • Consumer Goods
  • Industrial Applications
General Information
Additive
  • Heat Stabilizer
  • Plasticizer
Features
  • Good Flexibility
  • Good Impact Resistance
  • Heat Stabilized
  • High Viscosity
  • Plasticized
Uses
  • Automotive Applications
  • Consumer Applications
  • Hydraulic Applications
  • Industrial Applications
  • Pneumatic Applications
RoHS Compliance
  • RoHS Compliant
Forms
  • Granules
Processing Method
  • Extrusion
PhysicalDryConditionedUnitTest Method
Density 1.01--g/cm³ISO 1183
Molding Shrinkage ISO 294-4
     Across Flow 1.2--%
     Flow 0.80--%
Water Absorption ISO 62
     Saturation, 23°C 1.5--%
     Equilibrium, 23°C, 50% RH 0.70--%
HardnessDryConditionedUnitTest Method
Shore Hardness (Shore D, 15 sec)--67ISO 868
MechanicalDryConditionedUnitTest Method
Tensile Modulus --600MPaISO 527-2
Tensile Stress ISO 527-2
     Yield --35.0MPa
     Break --40.0MPa
Tensile Strain ISO 527-2
     Yield --15%
     Break > 50--%
Nominal Tensile Strain at Break --> 50%ISO 527-2
ImpactDryConditionedUnitTest Method
Charpy Notched Impact Strength ISO 179/1eA
     -30°C --7.0kJ/m²
     23°C --95kJ/m²
Charpy Unnotched Impact Strength ISO 179/1eU
     -30°C No BreakNo Break
     23°C No BreakNo Break
ThermalDryConditionedUnitTest Method
Heat Deflection Temperature
     0.45 MPa, Unannealed 115--°CISO 75-2/B
     1.8 MPa, Unannealed 45.0--°CISO 75-2/A
Continuous Use Temperature Internal Method
     -- 180.0 to 120--°C
     -- 2150--°C
Melting Temperature 3175--°CISO 11357-3
CLTE ISO 11359-2
     Flow 1.3E-4--cm/cm/°C
     Transverse 1.6E-4--cm/cm/°C
ElectricalDryConditionedUnitTest Method
Surface Resistivity --1.0E+12ohmsIEC 60093
Volume Resistivity --1.0E+13ohms·cmIEC 60093
Electric Strength --32kV/mmIEC 60243-1
Comparative Tracking Index --600VIEC 60112
FlammabilityDryConditionedUnitTest Method
Flammability Classification (0.800 mm)HB--IEC 60695-11-10, -20
Additional InformationDryConditionedTest Method
ISO Type PA12-HIP, EHL, 22-007--ISO 1874
Note Message
1 .Long Term
2 .Short Term
3 .10°C/min
Resin Grade Manufacturer Category Trademark
TECHNO ALPHALOY MPA G101 Techno Polymer Co, Ltd. ABS+Nylon TECHNO ALPHALOY
I. Stern 728 I. STERN & CO. INC. ABS I. Stern
Lifoflex® UV 20 GC 1020 ELASTO SEBS Lifoflex®
LUVOCOM® 80-8999/BL/L Lehmann & Voss & Co. Acetal (POM) Copolymer LUVOCOM®
PENTAMID A SK H natur PENTAC Polymer GmbH Nylon 66 PENTAMID A