MAXAMID™ EPDMRC0366-HSL-BK09

Category: Nylon 66 , Polyamide 66
Manufacturer: Pier One Polymers, Inc.
Trademark: MAXAMID™
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: 9BwMxs_MAXAMIDEPDMRC0366HSLBK09.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
MAXAMID™ EPDMRC0366HSL is available in black only with internal and external lubricants, UV stabilized and other modifications available. Manufactured with recycled content. Further information and details are available upon request.
General Information
Additive
  • Impact modifier
  • Lubricant
  • UV stabilizer
Recycled Content
  • Yes
Features
  • UV Stabilized
  • Impact modification
  • Lubrication
Appearance
  • Black
Forms
  • Particle
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.09g/cm³ASTM D792
MechanicalNominal ValueUnitTest Method
Tensile Strength (23°C)59.3MPaASTM D638
Tensile Elongation (Break, 23°C)40%ASTM D638
Flexural Modulus (23°C)2140MPaASTM D790
Flexural Strength (23°C)84.1MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (23°C)160J/mASTM D256
ThermalNominal ValueUnitTest Method
Deflection Temperature Under Load (1.8 MPa, Unannealed)72.0°CASTM D648
Peak Melting Temperature 255°CASTM D3418
InjectionNominal ValueUnit
Suggested Max Moisture 0.20%
Processing (Melt) Temp 290 - 305°C
Mold Temperature 38 - 93°C
Resin Grade Manufacturer Category Trademark
Manner Flexible PVC M1160 Manner Plastics, L.P. PVC, Flexible Manner Flexible PVC
Michilene F8100 API Polymers, Inc. PP Homopolymer Michilene
Desmopan® 487 Covestro - PUR TPU-Polyester Desmopan®
ExxonMobil™ LDPE LD 103 Series ExxonMobil Chemical LDPE ExxonMobil™ LDPE
Sylvin 6248-80 Yellow 4177 Sylvin Technologies Incorporated PVC, Unspecified Sylvin