Category: | HDPE , High Density Polyethylene Solid Insulation Compound |
Manufacturer: | The Dow Chemical Company |
Trademark: | AXELERON™ |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 8tiahs_AXELERON-CS-L-3364-NT-CPD.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
AXELERON™ CS L-3364 NT CPD is a high-molecular weight, high-density polyethylene insulation compound ("CPD") specifically formulated to provide excellent oxidative stability, toughness, and abrasion resistance. It provides superior long term aging performance, especially in the more demanding grease-filled cable applications while providing excellent environmental and thermal stress-cracking resistance. In addition, AXELERON™ CS L-3364 NT CPD provides excellent processibility for high-speed wire insulating extrusion processes. AXELERON™ CS L-3364 NT CPD provides excellent performance across the full range of telephone insulation applications, including aircore and grease-filled cable designs in both buried and aerial environments AXELERON™ CS L-3364 NT CPD is optimized to meet rigorous Telcordia (formerly Bellcore) age testing requirements, as well as all major international age testing standards and specifications for both solid and foam/skin insulation use. There is also considerable AXELERON™ CS L-3364 NT CPD use in a wide variety of other twisted pair, optic, coaxial and power cable designs. Specifications AXELERON™ CS L-3364 NT CPD meets the following raw material specifications:
Telephone wire insulated with AXELERON™ CS L-3364 NT CPD, using sound commercial extrusion practices, should meet the following cable specifications:
|
General Information | |
---|---|
Uses |
|
Agency Ratings |
|
Forms |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 0.945 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 0.80 | g/10 min | ASTM D1238 |
Environmental Stress-Cracking Resistance (50°C, 100% Igepal, F0) | > 48.0 | hr | ASTM D1693 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | 23.4 | MPa | ASTM D638 |
Tensile Elongation (Break) | 500 | % | ASTM D638 |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile strength retention- 48 hrs (100°C) | 90 | % | ASTM D638 |
Elongation retention rate- 48 hrs (100°C) | 90 | % | ASTM D638 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat resistant stress crack- F0 | > 96 | hr | ASTM D2951 |
Oxidation Induction Time 1(200°C) | 170 | min | ASTM D4565 |
Brittleness Temperature 2 | -76.0 | °C | ASTM D746 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity (23°C) | > 1.0E+15 | ohms·cm | ASTM D257 |
Dielectric Constant 3(1 MHz) | 2.32 | ASTM D1531 | |
Dissipation Factor (1 MHz) | 6.0E-5 | ASTM D1531 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Melt Temperature | 218 - 260 | °C |
Extrusion instructions |
---|
AXELERON™ CS L-3364 NT CPD provides excellent surface finish and good output rates over a broad range of extrusion conditions. AXELERON™ CS L-3364 NT CPD is typically extruded at melt discharge temperatures ranging from 425 to 500°F (220 to 260°C) using conductor preheats ranging from 230 to 290°F (110 to 140°C). Specific extrusion conditions can be recommended only when the application, processing speed and processing equipment details are known. |
Note Message | |
---|---|
1 . | Aluminum pan O/T testing of 0.25 mm film samples 80°C ETPR cable type filler was used. |
2 . | F0 |
3 . | After 14 days Water Immersion at 23°C (73°F) |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Moplen EP500N | PolyMirae | PP Copolymer | Moplen |
TRIMID® N66-G33HL | Polymer Technology and Services, LLC | Nylon 66 | TRIMID® |
Chemraz XRZ | Greene, Tweed & Co. | Perfluoroelastomer | Chemraz |
Luran® S 777K | Styrolution | ASA | Luran® S |
SABIC® PC PC1800R resin | SABIC Innovative Plastics Asia Pacific | PC | SABIC® PC |