| Category: | PUR-Ether/TDI , Polyurethane (Polyether, TDI) |
| Manufacturer: | Chemtura |
| Trademark: | Adiprene® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 8Gsrgi_Adiprene-LFG-964A.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
ADIPRENE LFG 964A is a TDI-terminated polyether prepolymer that yields a 95 Shore A elastomer when cured with MBCA. The features of ADIPRENE LFG 964A include:
LFG 964A offers improved safety during handling and processing over conventional-type prepolymers due to the low content of free TDI. |
| General Information | |
|---|---|
| Features |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.15 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore D) | 95 to 98 | ASTM D2240 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ASTM D412 | ||
| 100% Strain | 11.7 | MPa | |
| 300% Strain | 23.4 | MPa | |
| Tensile Strength | 29.0 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 320 | % | ASTM D412 |
| Tear Strength (Split) | 2.8 | kN/m | ASTM D470 |
| Compression Set (70°C, 22 hr) | 45 | % | ASTM D395B |
| Rebound Resilience - Drop Ball | 43 | % |
| Thermoset | Nominal Value | Unit | |
|---|---|---|---|
| Pot Life | 7.5 | min | |
| Post Cure Time (100°C) | 16 | hr |
| Uncured Properties | Nominal Value | Unit | |
|---|---|---|---|
| Curing Time (100°C) | 0.50 | hr |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| MARPOL® LDF 720 | Marco Polo International, Inc. | LDPE | MARPOL® |
| RTP 300 TFE 15 SE | RTP Company | PC | RTP |
| DJSilicone NE-9330 | DONGJUE SILICONE (NANJING) CO., LTD | Silicone | DJSilicone |
| Sylvin 5211-85 Natural | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
| ESTOPLAST EP 2030BB12 | Ester Industries Ltd. | PBT | ESTOPLAST EP |