Category: | LLDPE , Black Linear Low Density Polyethylene Compound for Cable Jacketing |
Manufacturer: | The Dow Chemical Company |
Trademark: | AXELERON™ |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 7ignWO_AXELERON-GP-6059-BK-CPD.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
AXELERON™ GP 6059 BK CPD is a prime quality telephone cable black jacketing compound ("CPD"). It offers improved low temperature and high temperature performance plus excellent environmental stress-cracking resistance, outdoor weatherability, and toughness. Specifications AXELERON™ GP 6059 BK CPD meets the following raw material specifications:
Cable jacketed with AXELERON™ GP 6059 BK CPD, using sound commercial extrusion practices, should meet the following specifications:
|
General Information | |
---|---|
Uses |
|
Agency Ratings |
|
Forms |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.932 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 0.60 | g/10 min | ASTM D1238 |
Environmental Stress-Cracking Resistance 1(10% Igepal, F0) | > 1000 | hr | ASTM D1693 |
Carbon Black Content | 2.6 | % | ASTM D1603 |
Absorption Coefficient - (kAB/m) | > 400 | ASTM D3349 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Oxidation Induction Time (200°C) | 120 | min | ASTM D3895 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | |||
-- | 21.0 | MPa | IEC 60811-502 |
-- | 16.2 | MPa | ASTM D638 |
Tensile Elongation | |||
Fracture | 900 | % | IEC 60811-502 |
Fracture | 700 | % | ASTM D638 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Brittleness Temperature | ASTM D746 | ||
-- 2 | < -100 | °C | ASTM D746 |
-- 3 | < -76.0 | °C | ASTM D746 |
Electrical | Nominal Value | Test Method | |
---|---|---|---|
Dielectric Constant (1 MHz) | 2.48 | ASTM D1531 | |
Dissipation Factor (1 MHz) | 3.0E-4 | ASTM D1531 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Melt Temperature | 218 - 246 | °C |
Extrusion instructions |
---|
AXELERON™ GP 6059 BK CPD provides excellent surface finish and outstanding output rates over a broad range of conditions. For optimum results, use melt extrusion temperatures in the suggested range of 425 to 475°F (218 to 246°C).Hopper drying at 150-160°F (67-71°C) is recommended to remove moisture. |
Note Message | |
---|---|
1 . | Typical value per IEC 60811-406 > 1000 hrs. |
2 . | F50 |
3 . | Notched, F50 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Vital-Line SHE5205G | Teknor Apex Asia Pacific PTE. LTD. | PVC, Flexible | Vital-Line |
Unichem 4060 | Colorite Polymers | PVC, Unspecified | Unichem |
APEX® 3300-45NT | Teknor Apex Company | PVC, Flexible | APEX® |
Chemical Resources RPP 200CW | Chemical Resources, Inc. | PP Random Copolymer | Chemical Resources |
CYCOLOY™ MC8100 resin | SABIC Innovative Plastics | PC+ABS | CYCOLOY™ |