Andur 1-75 DP is a polyether based liquid isocyanate-terminated prepolymer. An elastomer with a hardness of 73-77 Shore D is obtained when this prepolymer is cured with Curene 442 [4,4'- methylene-bis (orthochloroaniline)]. Elastomers of lower hardness can be obtained by reaction with various polyols and their combination with Curene 442 and other diamines, and by the use of plasticizers.
General Information
Forms
  • Liquid
PhysicalNominal ValueUnitTest Method
Density 1.16g/cm³ASTM D1505
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shore D)75ASTM D2240
ElastomersNominal ValueUnitTest Method
Tensile Stress (100% Strain)38.6MPaASTM D412
Tensile Strength (Yield)51.0MPaASTM D412
Tensile Elongation (Break)260%ASTM D412
Bayshore Resilience 58%ASTM D2632
ThermosetNominal ValueUnit
Pot Life 2.5 - 3.0min
Demold Time (100°C)10min
Post Cure Time (100°C)16hr
Additional Information
Durometer Hardness, ASTM D2240, Shore D: 73 to 77Die C Tear, ASTM D1004: 860 pliAverage Split Tear, ASTM D1938: 280 pliStoichiometry Curative Level: 95%Mix Temperature: Andur 1-75 DP: 150-180°F Curene 442: 220-235°F
Resin Grade Manufacturer Category Trademark
RTP 1102 RTP Company PET RTP
Silopren® LSR 2020 Momentive Performance Materials Inc. Silicone Rubber, LSR Silopren®
ExxonMobil™ LDPE LD 156 Series ExxonMobil Chemical LDPE ExxonMobil™ LDPE
LEXAN™ HPX8REU resin SABIC Innovative Plastics Europe PC LEXAN™
Plaslube® PC / ABS 1000 Techmer Engineered Solutions PC+ABS Plaslube®