| Category: | TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester) |
| Manufacturer: | ResMart |
| Trademark: | ResMart Ultra |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 5LZasP_ResMart-Ultra-TPU-95A-ES.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Polyester based TPU Shore 95A hardness for injection molding or extrusion applications |
| General Information | |
|---|---|
| Agency Ratings |
|
| RoHS Compliance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.20 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness | ASTM D2240 | ||
| Shore A | 95 | ||
| Shore D | 55 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength | 37.9 | MPa | ASTM D638 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Elongation (Break) | 400 | % | ASTM D412 |
| Tear Strength | 120 | kN/m | ASTM D624 |
| Flammability | Nominal Value | Test Method | |
|---|---|---|---|
| Flame Rating | HB | UL 94 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature - Desiccant Dryer | 82.2 to 104 | °C | |
| Drying Time - Desiccant Dryer | 2.0 to 4.0 | hr | |
| Suggested Max Moisture | 0.010 | % | |
| Processing (Melt) Temp | 185 to 210 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| CompaMid® PA 6.6 GF 15 | DimeLika Plast GmbH | Nylon 66 | CompaMid® |
| ExxonMobil™ LLDPE LL 6201 Series | ExxonMobil Chemical | LLDPE | ExxonMobil™ LLDPE |
| Elastron® G G501.A60.B.PS | Elastron USA, Inc. | SEBS | Elastron® G |
| PETILEN G08-21T | PETKIM Petrokimya Holding A.S. | LDPE | PETILEN |
| Petrothene® NA362 | LyondellBasell Industries | LDPE | Petrothene® |