All properties based on Andur® 8000-AP cured with Curene® 280
General Information
Forms
  • Liquid
Processing Method
  • Casting
HardnessNominal ValueTest Method
Durometer Hardness (Shore A)67ASTM D2240
MechanicalNominal ValueUnitTest Method
Tensile Strength 6.89MPaASTM D638
Tensile Elongation (Break)380%ASTM D638
ElastomersNominal ValueUnitTest Method
Tensile Stress ASTM D412
    100% strain 2.24MPaASTM D412
    300% strain 4.83MPaASTM D412
Tear Strength
    -- 126.3kN/mASTM D624
    Cracking 4.4kN/mASTM D470
Compression Set 17%ASTM D395
ThermosetNominal ValueUnit
Pot Life 25min
Post Cure Time (23°C)72hr
Additional Information
Prepolymer NCO%: 3.3-3.7Grams Curene® 280 per 100 grams prepolymer: 22.2Rebound, %: 20Stoichiometry: 0.95Prepolymer Temperature, °F: 190-210Curene® 280 Temperature, °F: 158Post Cure Time, 212°F, hours: 16
InjectionNominal ValueUnit
Mold Temperature 107°C
Note Message
1 .C mould
Resin Grade Manufacturer Category Trademark
VESTAMID® Terra HS22 natural color Evonik Industries AG Nylon 610 VESTAMID® Terra
Formolene® 6550A Formosa Plastics Corporation, U.S.A. PP Impact Copolymer Formolene®
Ecobarrier® 2012 Noble Polymers Polyolefin, Unspecified Ecobarrier®
Plaslube® PA6/6 GF/M40 ML2 GY Techmer Engineered Solutions Nylon 66 Plaslube®
TECHNYL® C 218L V30 BLACK-J Solvay Engineering Plastics Nylon 6 TECHNYL®