Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | Grupa Azoty S.A. |
Trademark: | Tarnamid® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 57qXeg_Tarnamid-T-27-GF30-V2.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Tarnamid® T-27 GF30 V2 is a Polyamide 6 (Nylon 6) material filled with 30% glass fiber. It is available in Africa & Middle East, Asia Pacific, Europe, Latin America, or North America for injection molding. Important attributes of Tarnamid® T-27 GF30 V2 are:
Typical applications include:
|
General Information | |
---|---|
Filler / Reinforcement |
|
Features |
|
Uses |
|
Forms |
|
Processing Method |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.45 | -- | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (275°C/5.0 kg) | 35 | -- | g/10 min | ISO 1133 |
Molding Shrinkage | 0.20 | 1.1 | % | ISO 294-4 |
Water Absorption (23°C, 24 hr) | 0.80 | -- | % | ISO 62 |
Hardness | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Ball Indentation Hardness (H 358/30) | 230 | -- | MPa | ISO 2039-1 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus | 9500 | -- | MPa | ISO 527-2 |
Tensile Stress (Yield) | 140 | -- | MPa | ISO 527-2 |
Tensile Strain (Break) | 4.0 | -- | % | ISO 527-2 |
Flexural Modulus | 8000 | -- | MPa | ISO 178 |
Flexural Stress (3.5% Strain) | 200 | -- | MPa | ISO 178 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength | 10 | -- | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength | 70 | -- | kJ/m² | ISO 179/1eU |
Notched Izod Impact Strength | 12 | -- | kJ/m² | ISO 180 |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 200 | -- | °C | ISO 75-2/A |
Vicat Softening Temperature | 210 | -- | °C | ISO 306/B50 |
Flammability | Dry | Conditioned | Test Method | |
---|---|---|---|---|
Flame Rating (3.20 mm) | V-2 | -- | UL 94 |
Injection | Dry | Unit | |
---|---|---|---|
Drying Temperature | 80.0 to 100 | °C | |
Drying Time | 2.0 to 4.0 | hr | |
Suggested Max Moisture | 0.20 | % | |
Processing (Melt) Temp | 250 to 290 | °C | |
Mold Temperature | 80.0 to 120 | °C | |
Injection Pressure | 80.0 to 130 | MPa | |
Injection Rate | Moderate |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
MTEGRITY™ PP Homopolymer PP410 | M. Holland Company | PP Homopolymer | MTEGRITY™ PP Homopolymer |
Borclean™ HC300BF | Borealis AG | PP Homopolymer | Borclean™ |
HiFill® PA6 0254 B2 | Techmer Engineered Solutions | Nylon 6 | HiFill® |
HOPELEX PCN-2001W | Lotte Chemical Corporation | PC | HOPELEX |
SABIC® FORTIFY™ C1085 | Saudi Basic Industries Corporation (SABIC) | TPO (POE) | SABIC® FORTIFY™ |