| Category: | SBS , Styrene Butadiene Styrene Block Copolymer |
| Manufacturer: | AKelastomers |
| Trademark: | Asaprene™ |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 4HSq8e_Asaprene-T-411.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| High molecular weight, for enhanced adhesive characteristics in pressure-sensitive and other adhesives and heightened softening point in asphalts. It is supplied in crumb or powder form. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.940 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) | ISO 1133 | ||
| 190°C/2.16 kg | 0.0 | g/10 min | |
| 200°C/5.0 kg | 0.0 | g/10 min | |
| Styrene/Butadiene | 30/70 | % | Internal Method |
| Viscosity | Internal Method | ||
| 10% solution in toluene | 270 | mPa·s | |
| 25% solution in toluene | 20200 | mPa·s |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Shore Hardness (Shore A, 23°C, 2.00 mm, Compression Molded) | 75 | ISO 7619 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress 1(300% Strain, 23°C, 2.00 mm) | 2.30 | MPa | ISO 37 |
| Tensile Stress 2(Break, 23°C, 2.00 mm) | 20.0 | MPa | ISO 37 |
| Tensile Elongation 3(Break, 23°C, 2.00 mm) | 750 | % | ISO 37 |
| Note Message | |
|---|---|
| 1 . | Type 1A |
| 2 . | Type 1A |
| 3 . | Type 1A |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| VESTOSINT® 2159 natural color | Evonik Industries AG | Nylon 12 | VESTOSINT® |
| Wellamid® GFT15N050-BK2 | Wellman Engineering Resins | Nylon 66 | Wellamid® |
| 4MID® 9B22145 | 4Plas | Nylon 6 | 4MID® |
| Haysite BMC 18600 | Haysite Reinforced Plastics | Polyester, TS | Haysite BMC |
| Polifor® 5210/V2 NATURALE | SO.F.TER. SPA | PP Homopolymer | Polifor® |