Type: Estane® 58810 TPU is a 90A Polyether-Type thermoplastic polyurethane Description: High melt flow and improved temperature resistance Uses: Extrusion - Wire and cable, Hose and tube |
General Information | |
---|---|
Features |
|
Uses |
|
RoHS Compliance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.13 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A, 5 sec) | 87 - 93 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Flexural Modulus (23°C) | 37.7 | MPa | ASTM D790 |
Taber Abrasion Resistance (1000 Cycles, 1000 g, H-18 Wheel) | 41.0 | mg | ASTM D3389 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ASTM D412 | ||
100% strain, 0.762mm | 9.00 | MPa | ASTM D412 |
300% strain, 0.762mm | 17.2 | MPa | ASTM D412 |
Tensile Strength (Break, 0.762 mm) | 38.3 | MPa | ASTM D412 |
Tensile Elongation (Break, 0.762 mm) | 530 | % | ASTM D412 |
Tear Strength | |||
0.762 mm 1 | 59.8 | kN/m | ASTM D624 |
Cracking | 18 | kN/m | ASTM D470 |
Compression Set | ASTM D395 | ||
23°C, 22 hr | 25 | % | ASTM D395 |
70°C, 22 hr | 60 | % | ASTM D395 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Glass Transition Temperature | -44.0 | °C | DSC |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 104 | °C | |
Drying Time | 2.0 - 4.0 | hr | |
Suggested Max Moisture | 0.020 | % | |
Cylinder Zone 1 Temp. | 176 | °C | |
Cylinder Zone 2 Temp. | 182 | °C | |
Cylinder Zone 3 Temp. | 191 | °C | |
Cylinder Zone 4 Temp. | 196 | °C | |
Adapter Temperature | 199 | °C | |
Melt Temperature | 196 | °C | |
Die Temperature | 194 - 196 | °C |
Extrusion instructions |
---|
Dew Point: -40°CScreen Pack Recommendation: 20/40/80/20 |
Note Message | |
---|---|
1 . | C mould |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Marlex® HMN TR-935 | Chevron Phillips Chemical Company LLC | MDPE | Marlex® |
Nipol® AR 51 | Zeon Corporation | Rubber | Nipol® AR |
Nylene® 4004 HS | Custom Resins Group | Nylon 6 | Nylene® |
Leona™ 13G25 | Asahi Kasei Chemicals Corporation | Nylon 66 | Leona™ |
SABIC® PPcompound 8503 | Saudi Basic Industries Corporation (SABIC) | PP, Unspecified | SABIC® PPcompound |