Category: | TPE , Thermoplastic Elastomer |
Manufacturer: | Teknor Apex Company |
Trademark: | Sarlink® TPE |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 3WTvpb_Sarlink-TPE-EE-2240N.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
The Sarlink EE-2200 series UV Resistant extrusion grades suitable for automotive exterior applications. |
General Information | |
---|---|
Additive |
|
Features |
|
Uses |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.17 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 0.40 | g/10 min | ASTM D1238 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness | ASTM D2240 | ||
Shaw A | 43 | ASTM D2240 | |
Shaw A, 15 seconds | 40 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ASTM D412 | ||
Transverse flow : 100% strain | 0.758 | MPa | ASTM D412 |
Flow : 100% strain | 1.17 | MPa | ASTM D412 |
Tensile Strength | ASTM D412 | ||
Transverse flow : Fracture | 5.79 | MPa | ASTM D412 |
Flow : Fracture | 3.59 | MPa | ASTM D412 |
Tensile Elongation | ASTM D412 | ||
Transverse flow : Fracture | 910 | % | ASTM D412 |
Flow : Fracture | 720 | % | ASTM D412 |
Tear Strength - Across Flow | 20.8 | kN/m | ASTM D624 |
Compression Set | ASTM D395 | ||
23°C, 22 hr | 11 | % | ASTM D395 |
70°C, 22 hr | 26 | % | ASTM D395 |
125°C, 70 hr | 78 | % | ASTM D395 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Rear Temperature | 199 - 210 | °C | |
Middle Temperature | 204 - 216 | °C | |
Front Temperature | 210 - 221 | °C | |
Nozzle Temperature | 216 - 227 | °C | |
Processing (Melt) Temp | 216 - 227 | °C | |
Mold Temperature | 35.0 - 65.6 | °C | |
Injection Pressure | 1.38 - 6.89 | MPa | |
Injection Rate | Fast | ||
Back Pressure | 0.172 - 0.862 | MPa | |
Screw Speed | 50 - 120 | rpm | |
Cushion | 3.81 - 25.4 | mm |
Injection instructions |
---|
Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C). |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Cylinder Zone 1 Temp. | 193 - 204 | °C | |
Cylinder Zone 2 Temp. | 199 - 210 | °C | |
Cylinder Zone 3 Temp. | 204 - 216 | °C | |
Cylinder Zone 5 Temp. | 210 - 221 | °C | |
Die Temperature | 216 - 227 | °C |
Extrusion instructions |
---|
Screw Speed: 30 to 100 rpm |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
SCANAMID 6 B12^ F25 | Polykemi AB | Nylon 6 | SCANAMID 6 |
Alkatuff® LL711UV | Qenos Pty Ltd | LLDPE | Alkatuff® |
Delta LDPE 20018 | Delta Polymers | LDPE | Delta |
KEBAFORM® C 904 CF | BARLOG plastics GmbH | Acetal (POM) Copolymer | KEBAFORM® C |
Lupoy® ER5001RFA | LG Chem Ltd. | PC+ABS | Lupoy® |