Elexar EL-8614A is a high performance thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. Elexar EL-8614A is a RoHS compliant, flame retardant grade suitable for both injection molding and extrusion.
General Information
Features
  • High specific gravity
  • High density
  • Workability, good
  • Good formability
  • Good coloring
  • Good adhesion
  • Low liquidity
  • Halogenated
  • Good chemical resistance
  • Good toughness
  • Fill
  • High hardness
  • Flame retardancy
Uses
  • Underground cable
  • Cable sheath
  • Electrical wire sheath material
  • Electrical conductor insulation material
  • Wire and cable applications
  • Wire sheath
  • Industrial cable insulation material
  • Connector
  • cord sheath
  • Terminal cable sheath material
RoHS Compliance
  • RoHS compliance
Appearance
  • Opacity
  • Available colors
Forms
  • Particle
Processing Method
  • Extrusion
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.16g/cm³ASTM D792
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg)4.0g/10 minASTM D1238
HardnessNominal ValueUnitTest Method
Durometer Hardness ASTM D2240
    Shaw D, 1 sec 60ASTM D2240
    Shaw D, 5 seconds 58ASTM D2240
ElastomersNominal ValueUnitTest Method
Tensile Stress ASTM D412
    100% strain 7.45MPaASTM D412
    300% strain 8.41MPaASTM D412
Tensile Strength (Yield)21.0MPaASTM D412
Tensile Elongation (Break)620%ASTM D412
AgingNominal ValueUnitTest Method
Change in Tensile Strength in Air (136°C, 168 hr)-26%ASTM D573
Change in Ultimate Elongation in Air (136°C, 168 hr)-26%ASTM D573
Change in Tensile Strength (60°C, 168 hr, in IRM 902 Oil)-36%ASTM D471
Change in Ultimate Elongation (60°C, 168 hr, in IRM 902 Oil)-12%ASTM D471
ThermalNominal ValueUnitTest Method
Brittleness Temperature -33.0°CASTM D746
ElectricalNominal ValueUnitTest Method
Volume Resistivity (23°C)8.5E+16ohms·cmASTM D257
Dielectric Constant ASTM D150
    25°C, 1 kHz 2.40ASTM D150
    25°C, 1 MHz 2.40ASTM D150
Dissipation Factor ASTM D150
    25°C, 1 kHz 9.4E-3ASTM D150
    25°C, 1 MHz 3.8E-3ASTM D150
FlammabilityNominal ValueUnitTest Method
Flame Rating (3.0 mm, Natural Color)V-0UL 94
Legal statement
The information and recommendations contained in this bulletin are, to the best of our knowledge, accurate and reliable but no guarantee of their accuracy is made. All products are sold upon condition that purchasers shall make their own tests to determine the suitability of such products for their particular purposes and uses and purchaser assumes all risks and liability for the results of use of the products, including use in accordance with seller's recommendations. Nothing in this bulletin constitutes permission or a recommendation to practice or use any invention covered by any patent owned by this company or others. There is no warranty of merchantability and there are no other warranties for the products described. For detailed Product Stewardship information, please contact us. Any product of Teknor Apex, including product names, shall not be used or tested in medical or food contact applications without the prior written acknowledgement of Teknor Apex as to the intended use. Please note that some products may not be available in one or more countries.
InjectionNominal ValueUnit
Rear Temperature 199 - 216°C
Middle Temperature 213 - 221°C
Front Temperature 221 - 227°C
Nozzle Temperature 221 - 229°C
Processing (Melt) Temp 221 - 229°C
Mold Temperature 25 - 66°C
Injection Pressure 1.38 - 6.89MPa
Injection Rate Moderate-Fast
Back Pressure 0.172 - 0.345MPa
Screw Speed 50 - 100rpm
Cushion 3.81 - 25.4mm
Injection instructions
Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C).
ExtrusionNominal ValueUnit
Cylinder Zone 1 Temp. 193 - 210°C
Cylinder Zone 2 Temp. 199 - 216°C
Cylinder Zone 3 Temp. 213 - 221°C
Cylinder Zone 4 Temp. 213 - 221°C
Cylinder Zone 5 Temp. 221 - 227°C
Die Temperature 221 - 229°C
Extrusion instructions
Screw Speed: 30 to 100 rpm
Resin Grade Manufacturer Category Trademark
RTP 2585 FR RTP Company PC+ABS RTP
Tempalux® Unfilled Westlake Plastics Company PEI Tempalux®
DIC.PPS FZL-4033 DIC Corporation PPS DIC.PPS
FHR Polypropylene P4C5N-046 Flint Hills Resources, LP PP Homopolymer FHR Polypropylene
OmniPro™ HPP CCF10 OMNI Plastics, LLC PP Homopolymer OmniPro™