Category: | PUR-Eth,aliphat , Polyurethane (Polyether, Aliphatic) |
Manufacturer: | Anderson Development Company |
Trademark: | Andur |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 2t7Qe1_Andur-AL-62-DP-Curene-110.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Andur AL 62 DP is a polyether (PTMG) based prepolymer terminated with an aliphatic isocyanate to improve color stability, hydrolytic stability, and give longer pot life. |
General Information | |
---|---|
Features |
|
Forms |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.06 | g/cm³ | ASTM D1505 |
Molding Shrinkage - Flow | 1.7 | % | ASTM D955 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore D) | 62 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (100% Strain) | 20.7 | MPa | ASTM D412 |
Tensile Strength (Yield) | 42.7 | MPa | ASTM D412 |
Tensile Elongation (Break) | 270 | % | ASTM D412 |
Bayshore Resilience | 50 | % | ASTM D2632 |
Thermoset | Nominal Value | Unit | |
---|---|---|---|
Pot Life | 3.8 | min | |
Demold Time (100°C) | 30 | min | |
Post Cure Time | |||
21°C | 72 | hr | |
100°C | 16 | hr |
Additional Information |
---|
Durometer Hardness, ASTM D2240, Shore D: 60 to 64Die C Tear, ASTM D1004: 470 pliAverage Split Tear, ASTM D1938: 135 pliStoichiometry Curative Level: 95%Mix Temperature: Andur AL 62 DP: 180°F Curene 110: 70°F |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Spartech Polycom SCR1F-4009 | Spartech Polycom | ABS | Spartech |
Sylvin 2957-80 White 1437 | Sylvin Technologies Incorporated | PVC, Flexible | Sylvin |
ASI POLYPROPYLENE PP 2407-01 | A. Schulman Inc. | PP Impact Copolymer | ASI POLYPROPYLENE |
FRIANYL® A3 GF20 V2XI | Nilit Plastics | Nylon 66 | FRIANYL® |
MAJORIS CT200 | AD majoris | PP, Unspecified | MAJORIS |