| Category: | Plastomer , Ethylene-based Plastomer |
| Manufacturer: | ICO Polymers EMEA, A Division of A. Schulman |
| Trademark: | ICORENE® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 2OqWKY_ICORENE-N2004.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
ICORENE N2004 is an ethylene based octene plastomer produced using a metallocene catalyst. ICORENE® N2004 is designed for applications requiring excellent flow, high flexibility, outstanding toughness and excellent low temperature impact. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.902 | g/cm³ | ASTM D1505 |
| Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 30 | g/10 min | ASTM D1238 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore D) | 34 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (Break) | 13.0 | MPa | ASTM D638 |
| Tensile Elongation (Break) | 1300 | % | ASTM D638 |
| Flexural Modulus | 67.0 | MPa | ASTM D790 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Vicat Softening Temperature | 72.0 | °C | ASTM D1525 |
| Peak Melting Temperature | 97.0 | °C | ASTM D3418 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP ESD C 260H | RTP Company | Nylon 66 | RTP |
| SLOVAMID® 6 BT | Plastcom | Nylon 6 | SLOVAMID® 6 |
| YUNGSOX® PP 3040C | Formosa Polypropylene | PP Impact Copolymer | YUNGSOX® PP |
| ExxonMobil™ LLDPE LL 1001 Series | ExxonMobil Chemical | LLDPE | ExxonMobil™ LLDPE |
| NORYL™ GFN3 resin | SABIC Innovative Plastics | PPE+PS | NORYL™ |