| Mineral reinforced |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Physical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Density | 2.00 | -- | g/cm³ | ISO 1183 |
| Mechanical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Tensile Stress | -- | 73.0 | MPa | ISO 527-2 |
| Tensile Strain | ISO 527-2 | |||
| Yield | -- | 5.0 | % | |
| Break | -- | 5.8 | % | |
| Flexural Modulus (23°C) | -- | 4900 | MPa | ISO 178 |
| Flexural Stress | -- | 100 | MPa | ISO 178 |
| Impact | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179 | |||
| -20°C | 3.5 | -- | kJ/m² | |
| 23°C | -- | 4.0 | kJ/m² |
| Thermal | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Heat Deflection Temperature 1 | ||||
| 0.45 MPa, Unannealed | 190 | -- | °C | ISO 75-2/B |
| 1.8 MPa, Unannealed | 93.0 | -- | °C | ISO 75-2/A |
| Vicat Softening Temperature | ||||
| -- | 225 | -- | °C | ISO 306/A50 |
| -- | 213 | -- | °C | ISO 306/B50 |
| Note Message | |
|---|---|
| 1 . | 120°C/hr |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| ENSOFT SO-160-45A | ENPLAST, a Ravago Group Company | TPE | ENSOFT |
| Escorene™ Ultra FL 00112 | ExxonMobil Chemical | EVA | Escorene™ Ultra |
| LNP™ LUBRICOMP™ CX94108 compound | SABIC Innovative Plastics Europe | PS (HIPS) | LNP™ LUBRICOMP™ |
| Lotrène® LDPE FE8000 | QAPCO | LDPE | Lotrène® LDPE |
| POCAN® B 3215 XF 000000 | LANXESS Asia/Pacific | PBT | POCAN® |