Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | EMS-GRIVORY |
Trademark: | Grilon® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 1mObXo_Grilon-BFZ-3.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Grilon® BFZ 3 is a Polyamide 6 (Nylon 6) material. It is available in Africa & Middle East, Asia Pacific, Europe, Latin America, or North America for blow molding, extrusion, injection molding, or injection stretch blow molding. Important attributes of Grilon® BFZ 3 are:
Typical applications include:
|
General Information | |
---|---|
Additive |
|
Features |
|
Uses |
|
Agency Ratings |
|
RoHS Compliance |
|
Forms |
|
Processing Method |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.06 | -- | g/cm³ | ISO 1183 |
Molding Shrinkage | ISO 294-4 | |||
Across Flow | 1.4 | -- | % | |
Flow | 1.1 | -- | % | |
Water Absorption | ISO 62 | |||
Saturation, 23°C | 9.0 | -- | % | |
Equilibrium, 23°C, 50% RH | 3.0 | -- | % |
Hardness | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Ball Indentation Hardness | 95.0 | 40.0 | MPa | ISO 2039-1 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus | 1800 | 600 | MPa | ISO 527-2 |
Tensile Stress (Yield) | 50.0 | 25.0 | MPa | ISO 527-2 |
Tensile Strain (Yield) | 4.0 | 15 | % | ISO 527-2 |
Nominal Tensile Strain at Break | > 50 | > 50 | % | ISO 527-2 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | |||
-30°C | 15 | 15 | kJ/m² | |
23°C | 65 | 120 | kJ/m² | |
Charpy Unnotched Impact Strength | ISO 179/1eU | |||
-30°C | No Break | No Break | ||
23°C | No Break | No Break |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature | ||||
0.45 MPa, Unannealed | 130 | -- | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 50.0 | -- | °C | ISO 75-2/A |
Continuous Use Temperature | Internal Method | |||
-- 1 | 80.0 to 110 | -- | °C | |
-- 2 | 160 | -- | °C | |
Melting Temperature 3 | 222 | -- | °C | ISO 11357-3 |
CLTE | ISO 11359-2 | |||
Flow | 1.3E-4 | -- | cm/cm/°C | |
Transverse | 1.5E-4 | -- | cm/cm/°C |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Surface Resistivity | -- | 1.0E+12 | ohms | IEC 60093 |
Volume Resistivity | 1.0E+14 | 1.0E+13 | ohms·cm | IEC 60093 |
Electric Strength | 42 | 39 | kV/mm | IEC 60243-1 |
Comparative Tracking Index | -- | 600 | V | IEC 60112 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Flammability Classification (0.800 mm) | HB | -- | IEC 60695-11-10, -20 |
Additional Information | Dry | Conditioned | Test Method | |
---|---|---|---|---|
ISO Type | PA6-HI, MHR, 18-020N | -- | ISO 1874 |
Note Message | |
---|---|
1 . | Long Term |
2 . | Short Term |
3 . | 10°C/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 4099 X 123510 A | RTP Company | PPA | RTP |
ADLEN® G08BGD00 | A.D. Compound S.p.A. | PP Copolymer | ADLEN® |
Osterlene® HD0860 | Osterman & Company | HDPE | Osterlene® |
ESTOPLAST EP 1500GY164 | Ester Industries Ltd. | PBT | ESTOPLAST EP |
CYCOLAC™ DL100 resin | SABIC Innovative Plastics Europe | ABS | CYCOLAC™ |