A special thermoplastic polyolefin resin with good rigidity/toughness balance, suitable for automotive exterior parts (such as bumper panels). |
General Information | |
---|---|
Features |
|
Uses |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.980 | g/cm³ | ISO 1183 |
Melt Volume-Flow Rate (MVR) | 19.0 | cm³/10min | ISO 1133 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus - Secant (23°C) | 1200 | MPa | ISO 527-2 |
Tensile Stress | ISO 527-2 | ||
Yield | 15.1 | MPa | ISO 527-2 |
Fracture | 11.6 | MPa | ISO 527-2 |
Tensile Strain | ISO 527-2 | ||
Yield | 4.3 | % | ISO 527-2 |
Fracture | 79 | % | ISO 527-2 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | ||
-30°C, complete fracture | 8.0 | kJ/m² | ISO 179 |
-20°C, complete fracture | 11 | kJ/m² | ISO 179 |
23°C, local fracture | 65 | kJ/m² | ISO 179 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 47.0 | °C | ISO 75-2/A |
Legal statement |
---|
本产品不宜在与食品接触的应用中使用。本产品不宜在医疗应用中使用,亦不应在任何此类应用中使用 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
NORYL™ NC212 resin | SABIC Innovative Plastics Asia Pacific | PPE+PS | NORYL™ |
Flontech® FT-CARR25-FM-3 | Guarniflon S.p.A. - Flontech Division | PTFE | Flontech® |
Sylvin 8960-70 Black | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
PERSTIR® N09K7000AE0 | A.D. Compound S.p.A. | PS (GPPS) | PERSTIR® |
Rotec® ABS 1200 TR-AC | ROMIRA GmbH | ABS | Rotec® ABS |