Molding Parameters:
The dry temperature at 16 hours is 250°F.
For 2-zone machines, the rear temperature is 600-640°F, and the front temperature is 580-600°F.
General Information
Filler / Reinforcement
  • Glass Fiber, 40% Filler by Weight
Features
  • Chemically Coupled
  • Flame Retardant
  • High Strength
RoHS Compliance
  • RoHS Compliant
Forms
  • Pellets
Processing Method
  • Injection Molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.68g/cm³ASTM D792
Molding Shrinkage - Flow 0.10%ASTM D955
Water Absorption (24 hr)0.020%ASTM D570
HardnessNominal ValueUnitTest Method
Rockwell Hardness (M-Scale)93ASTM D785
MechanicalNominal ValueUnitTest Method
Tensile Modulus 15200MPaASTM D638
Tensile Strength (Yield)165MPaASTM D638
Tensile Elongation (Yield)1.3%ASTM D638
Flexural Modulus 14500MPaASTM D790
Flexural Strength (Yield)231MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (23°C, 3.18 mm)91J/mASTM D256
ThermalNominal ValueUnitTest Method
Deflection Temperature Under Load (1.8 MPa, Unannealed)260°CASTM D648
InjectionNominal ValueUnit
Drying Temperature 163°C
Drying Time 4.0hr
Suggested Max Moisture 0.020%
Rear Temperature 288 to 304°C
Middle Temperature 316 to 343°C
Front Temperature 310 to 332°C
Nozzle Temperature 316 to 332°C
Processing (Melt) Temp 324 to 338°C
Mold Temperature 129 to 163°C
Resin Grade Manufacturer Category Trademark
Ravamid® A MF30 BK45 Ravago Group Nylon 66 Ravamid®
TOTAL Polystyrene Compound 818R TOTAL Refining & Chemicals PS (Specialty) TOTAL Polystyrene
ENPRENE 9840 En Chuan Chemical Industries Co,. Ltd. SBS ENPRENE
KOPLA PP KPR1166 KOPLA Co., Ltd. PP, Unspecified KOPLA PP
KOPLA PP KPT1040 KOPLA Co., Ltd. PP, Unspecified KOPLA PP