Category: | Nylon 612 , Polyamide 612 |
Manufacturer: | RTP Company |
Trademark: | RTP |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 1ck39L_RTP-281D-TFE-15-FR.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Warning: The status of this material is 'Commercial: Limited Issue' The data for this material has not been recently verified. Please contact RTP Company for current information prior to specifying this grade. -Preliminary Product Data per RTP Co.- |
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.55 | g/cm³ | ASTM D792 |
Molding Shrinkage - Flow (3.18 mm) | 0.30 | % | ASTM D955 |
Water Absorption (23°C, 24 hr) | 0.20 | % | ASTM D570 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Rockwell Hardness (R-Scale) | 118 | ASTM D785 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 9650 | MPa | ASTM D638 |
Tensile Strength | 96.5 | MPa | ASTM D638 |
Tensile Elongation (Break) | 1.0 | % | ASTM D638 |
Flexural Modulus | 8270 | MPa | ASTM D790 |
Flexural Strength | 165 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (3.18 mm) | 53 | J/m | ASTM D256 |
Unnotched Izod Impact (3.18 mm) | 370 | J/m | ASTM D4812 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load | ASTM D648 | ||
0.45 MPa, not annealed | 210 | °C | ASTM D648 |
1.8 MPa, not annealed | 199 | °C | ASTM D648 |
Flammability | Nominal Value | Test Method | |
---|---|---|---|
Flame Rating (1.59 mm) | V-0 | UL 94 |
Additional Information |
---|
Mold Shrinkage, Linear-Flow, ASTM D-955, 0.25in.: 4mil/in.Tensile Elongation, ASTM D-638: 1-2% |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 79.4 | °C | |
Drying Time | 4.0 | hr | |
Suggested Max Moisture | 0.20 | % | |
Suggested Max Regrind | 20 | % | |
Rear Temperature | 249 - 274 | °C | |
Middle Temperature | 249 - 274 | °C | |
Front Temperature | 249 - 274 | °C | |
Mold Temperature | 60.0 - 93.3 | °C | |
Injection Pressure | 103 - 138 | MPa |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 1407 Z | RTP Company | PESU | RTP |
Triapol® Blends F3 K55 VRD0241 BS305 | Petropol Industry and Trade of Polymers LTDA | PC+PBT | Triapol® Blends |
ALTECH® PA66 A 2060/100 GF60 | ALBIS PLASTIC GmbH | Nylon 66 | ALTECH® PA66 |
HiFill® PBT 1226 | Techmer Engineered Solutions | PBT | HiFill® |
KumhoSunny PC/ABS HAC8240 | Shanghai KumhoSunny Plastics Co., Ltd. | PC+ABS | KumhoSunny PC/ABS |