| Category: | TPO (POE) , Thermoplastic Polyolefin Elastomer |
| Manufacturer: | LyondellBasell Industries |
| Trademark: | Softell |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 0zSUGH_SoftellDKG100N.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Softell DKG100N is a 10% glass filled, thermoplastic polyolefin elastomer compound for injection molding. The grade has been designed primarily for automotive interior applications that require low gloss, soft touch, high rigidity, good impact and scratch and mar resistance. |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Features |
|
| Uses |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density (23°C) | 0.960 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 20 | g/10 min | ISO 1133 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Yield, 23°C) | 28.0 | MPa | ISO 527-2 |
| Tensile Strain (Yield, 23°C) | 10 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 1750 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact | ISO 180 | ||
| -30°C | 10 | kJ/m² | ISO 180 |
| 23°C | 30 | kJ/m² | ISO 180 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (0.45 MPa, Unannealed) | 140 | °C | ISO 75-2/B |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Prime Tuff-X 200 | Primex Plastics Corporation | Unspecified | Prime Tuff-X |
| RheTech Polypropylene T20P100-00UV | RheTech, Inc. | PP, Unspecified | RheTech Polypropylene |
| Tecnoprene® 3K3F NAT005 | SO.F.TER. SPA | PP Copolymer | Tecnoprene® |
| UBESTA 3030 JFX1 | UBE Engineering Plastics, S.A. | Nylon 12 | UBESTA |
| Kepamid® 1300CRK | Korea Engineering Plastics Co., Ltd | Nylon 6 | Kepamid® |