| Category: | EVA , Ethylene Vinyl Acetate Copolymer |
| Manufacturer: | Marco Polo International, Inc. |
| Trademark: | MARPOL® EVA |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 0v7BKm_MARPOLEVA3243.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
MARPOL® EVA 3243 is a Ethylene Vinyl Acetate copolymer resin designed for photovoltaic cells and encapsulation applications that require a good balance of adhesion and COF. It also exhibits excellent light transmission characteristics Recommended Applications: Encapsulation, hot melt adhesives and photovoltaic cells |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.954 | g/cm³ | |
| Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 43 | g/10 min | ASTM D1238 |
| Vinyl Acetate Content | 31.5 | wt% |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness | ASTM D2240 | ||
| Shaw A | 66 | ASTM D2240 | |
| Shaw D | 13 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 8.27 | MPa | ASTM D638 |
| Tensile Strength (Break) | 6.21 | MPa | ASTM D638 |
| Tensile Elongation (Break) | > 900 | % | ASTM D638 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Vicat Softening Temperature | 33.9 | °C | ASTM D1525 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 3400 G-430 | RTP Company | LCP | RTP |
| THERMOLAST® M TM5ADT (Series: MC/AD1) | KRAIBURG TPE | TPE | THERMOLAST® M |
| Evermore PUR UDA-10XT | Evermore Chemical Industry Co., Ltd. | PUR-Ether | Evermore PUR |
| Petrothene® NA426225 | LyondellBasell Industries | LDPE+EVA | Petrothene® |
| ESTOPLAST ZK 6002BB02 | Ester Industries Ltd. | PC | ESTOPLAST ZK |