Sarlink® TPE RV-2240

Category: TPE , Thermoplastic Elastomer
Manufacturer: Teknor Apex Company
Trademark: Sarlink® TPE
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: 0nkkRd_SarlinkTPERV2240.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Sarlink TPE RV-2240 is a high performance thermoplastic elastomer used in a variety of transportation applications. Sarlink TPE RV-2240 is a low hardness, low density extrusion grade with good UV resistance.


General Information
Features
  • Low Specific Gravity
  • Low density
  • smoothness
  • Light stabilization
  • Good UV resistance
  • Low liquidity
  • Lubrication
  • Fill
  • Hardness, low
Uses
  • Application in Automobile Field
  • Automotive exterior parts
  • Car exterior decoration
  • Rubber substitution
RoHS Compliance
  • RoHS compliance
Appearance
  • Black
  • Natural color
Forms
  • Particle
Processing Method
  • Extrusion
PhysicalNominal ValueUnitTest Method
Specific Gravity 0.948g/cm³ASTM D792
Melt Mass-Flow Rate (MFR) (200°C/5.0 kg)5.0g/10 minASTM D1238
HardnessNominal ValueUnitTest Method
Durometer Hardness ASTM D2240
    Shaw A, 1 sec 42ASTM D2240
    Shaw A, 5 seconds 40ASTM D2240
ElastomersNominal ValueUnitTest Method
Tensile Strength (Break)7.58MPaASTM D412
Tensile Elongation (Break)650%ASTM D412
Tear Strength 119.3kN/mASTM D624
Compression Set (70°C, 22 hr)28%ASTM D395
Legal statement
The information and recommendations contained in this bulletin are, to the best of our knowledge, accurate and reliable but no guarantee of their accuracy is made. All products are sold upon condition that purchasers shall make their own tests to determine the suitability of such products for their particular purposes and uses and purchaser assumes all risks and liability for the results of use of the products, including use in accordance with seller's recommendations. Nothing in this bulletin constitutes permission or a recommendation to practice or use any invention covered by any patent owned by this company or others. There is no warranty of merchantability and there are no other warranties for the products described. For detailed Product Stewardship information, please contact us. Any product of Teknor Apex, including product names, shall not be used or tested in medical or food contact applications without the prior written acknowledgement of Teknor Apex as to the intended use. Please note that some products may not be available in one or more countries.
Injection instructions
Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C).
ExtrusionNominal ValueUnit
Cylinder Zone 1 Temp. 160 - 204°C
Cylinder Zone 2 Temp. 166 - 210°C
Cylinder Zone 3 Temp. 171 - 216°C
Cylinder Zone 4 Temp. 171 - 216°C
Cylinder Zone 5 Temp. 177 - 221°C
Die Temperature 177 - 221°C
Extrusion instructions
Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C).;Screw Speed: 30 to 100 rpm
Note Message
1 .C mould
Resin Grade Manufacturer Category Trademark
Salflex 810C-2 Salflex Polymers Ltd. PP Copolymer Salflex
RheTech Polypropylene HP531-00 RheTech, Inc. PP Copolymer RheTech Polypropylene
XENOY™ X2420 resin SABIC Innovative Plastics Asia Pacific PC+Polyester XENOY™
KumhoSunny AES HW600G Shanghai KumhoSunny Plastics Co., Ltd. AES KumhoSunny AES
LNP™ STAT-KON™ OE006A compound SABIC Innovative Plastics PPS, Branched LNP™ STAT-KON™