Category: | TPV , Thermoplastic Vulcanizate |
Manufacturer: | ExxonMobil Chemical |
Trademark: | Santoprene™ |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 0OWqiY_Santoprene-8201-80.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
It is a soft, colorable, non-hygroscopic thermoplastic vulcanized elastomer (TPV) in the thermoplastic elastomer (TPE) series. This material has good physical properties and chemical resistance at the same time, and is suitable for a wide range of fields. This brand of Shanduping TPV is a shear rate dependent product that can be processed on conventional thermoplastic injection molding, extrusion molding, blow molding, thermoforming or vacuum forming equipment. This is a polyolefin-based material that can be recycled in the production process. |
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
RoHS Compliance |
|
UL File Number |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | |||
-- | 0.948 | g/cm³ | ASTM D792 |
-- | 0.950 | g/cm³ | ISO 1183 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shaw A, 15 seconds, 23°C, 2.00mm) | 85 | ISO 868 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress - Across Flow (100% Strain, 23°C) | 4.20 | MPa | ASTM D412, ISO 37 |
Tensile Strength - Across Flow (Break, 23°C) | 9.80 | MPa | ASTM D412, ISO 37 |
Tensile Elongation - Across Flow (Break, 23°C) | 630 | % | ASTM D412, ISO 37 |
Tear Strength - Across Flow | |||
23°C 1 | 43.0 | kN/m | ASTM D624 |
23°C 2 | 43 | kN/m | ISO 34-1 |
Compression Set | |||
70°C, 22 hr 3 | 35 | % | ASTM D395B |
125°C, 70 hr 4 | 69 | % | ASTM D395B |
70°C, 22 hr 5 | 35 | % | ISO 815 |
125°C, 70 hr 6 | 69 | % | ISO 815 |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Tensile Strength in Air (150°C, 168 hr) | -6.0 | % | ASTM D573, ISO 188 |
Change in Ultimate Elongation in Air (150°C, 168 hr) | -19 | % | ASTM D573, ISO 188 |
Change in Durometer Hardness in Air (Shore A, 150°C, 168 hr) | 1.0 | ASTM D573, ISO 188 | |
Change in Mass in Air (150°C, 168 hr) | -8.0 | % | ASTM D573 |
Change in Mass in Air (150°C, 168 hr) | -8.0 | % | ISO 188 |
Change in Tensile Strength | ASTM D471, ISO 1817 | ||
23°C, 168 hr, in 15% sodium chloride | -3.0 | % | ASTM D471, ISO 1817 |
23°C, 168 hr, in 50% sodium hydroxide | -3.0 | % | ASTM D471, ISO 1817 |
23°C, 168 hr, in 98% sulfuric acid | -4.0 | % | ASTM D471, ISO 1817 |
23°C, 168 hr, in IRM 903 oil | -15 | % | ASTM D471, ISO 1817 |
23°C, 168 hr, in water | 0.0 | % | ASTM D471, ISO 1817 |
Change in Ultimate Elongation | ASTM D471, ISO 1817 | ||
23°C, 168 hr, in 15% sodium chloride | -4.0 | % | ASTM D471, ISO 1817 |
23°C, 168 hr, in 50% sodium hydroxide | 0.0 | % | ASTM D471, ISO 1817 |
23°C, 168 hr, in 98% sulfuric acid | -6.0 | % | ASTM D471, ISO 1817 |
23°C, 168 hr, in IRM 903 oil | -8.0 | % | ASTM D471, ISO 1817 |
23°C, 168 hr, in water | 15 | % | ASTM D471, ISO 1817 |
Change in Durometer Hardness | |||
Support A, 23°C, 168 hr, in 15% sodium chloride | 1.0 | ASTM D471 | |
Support A, 23°C, 168 hr, in 50% sodium hydroxide | 2.0 | ASTM D471 | |
Support A, 23°C, 168 hr, in 98% sulfuric acid | 2.0 | ASTM D471 | |
Support A, 23°C, 168 hr, in IRM 903 oil | -11 | ASTM D471 | |
Support A, 23°C, 168 hr, in water | -1.0 | ASTM D471, ISO 1817 | |
Support A, 23°C, 168 hr, in 15% sodium chloride | 1.0 | ISO 1817 | |
Support A, 23°C, 168 hr, in 50% sodium hydroxide | 2.0 | ISO 1817 | |
Support A, 23°C, 168 hr, in 98% sulfuric acid | 2.0 | ISO 1817 | |
Support A, 23°C, 168 hr, in IRM 903 oil | -11 | ISO 1817 | |
Change in Mass | ASTM D471 | ||
23°C, 168 hr, in 15% sodium chloride | -1.0 | % | ASTM D471 |
23°C, 168 hr, in 50% sodium hydroxide | -1.0 | % | ASTM D471 |
23°C, 168 hr, in 98% sulfuric acid | 0.0 | % | ASTM D471 |
23°C, 168 hr, in IRM 903 oil | 36 | % | ASTM D471 |
23°C, 168 hr, in water | 2.0 | % | ASTM D471 |
Change in Mass | ISO 1817 | ||
23.0°C, 168 hr, in 15% sodium chloride | -1.0 | % | ISO 1817 |
23.0°C, 168 hr, in 50% sodium hydroxide | -1.0 | % | ISO 1817 |
23.0°C, 168 hr, in 98% sulfuric acid | 0.0 | % | ISO 1817 |
23.0°C, 168 hr, in water | 2.0 | % | ISO 1817 |
23.0°C, 168 hr, in IRM 903 oil | 36 | % | ISO 1817 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Brittleness Temperature | -63.0 | °C | ASTM D746, ISO 812 |
RTI Elec | 100 | °C | UL 746 |
RTI | UL 746 | ||
1.10 mm | 90.0 | °C | UL 746 |
1.60 mm | 90.0 | °C | UL 746 |
3.00 mm | 95.0 | °C | UL 746 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity | ASTM D257 | ||
23°C, 2.00 mm | 5.5E+17 | ohms·cm | ASTM D257 |
23°C, 3.20 mm | 2.4E+16 | ohms·cm | ASTM D257 |
Comparative Tracking Index (CTI) | PLC 0 | UL 746 | |
High Amp Arc Ignition (HAI) | PLC 0 | UL 746 | |
High Voltage Arc Resistance to Ignition (HVAR) | PLC 5 | UL 746 | |
Hot-wire Ignition (HWI) | UL 746 | ||
1.60 mm | PLC 3 | UL 746 | |
3.00 mm | PLC 2 | UL 746 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating | UL 94 | ||
1.10 mm | HB | UL 94 | |
1.60 mm | HB | UL 94 | |
3.00 mm | HB | UL 94 |
Additional Information |
---|
如果适用,这是基于扇形浇口注塑成型的平板测试结果。拉伸强度、伸长率和拉伸应力沿垂直流动方向测定 - ISO 1 型,ASTM die C。25% 形变时的永久压缩变形。从埃克森美孚欧洲分支机构直接购买的所有产品都符合 REACH 法规。 对于埃克森 美孚未进口至欧洲的产品,用户应自行评估其是否满足 REACH 法规。 |
Legal statement |
---|
未经埃克森美孚化工书面允许,这种产品包括其产品名称,不得在任何医疗应用领域予以使用或有关详细的产品监管信息,请联系客户服务。 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Suggested Max Moisture | 0.080 | % | |
Suggested Max Regrind | 20 | % | |
Rear Temperature | 185 - 199 | °C | |
Middle Temperature | 191 - 204 | °C | |
Front Temperature | 191 - 204 | °C | |
Nozzle Temperature | 199 - 216 | °C | |
Processing (Melt) Temp | 199 - 216 | °C | |
Mold Temperature | 23.9 - 51.7 | °C | |
Injection Rate | Fast | ||
Back Pressure | 0.345 - 0.689 | MPa | |
Screw Speed | 100 - 200 | rpm | |
Clamp Tonnage | 4.1 - 6.9 | kN/cm² | |
Cushion | 3.18 - 6.35 | mm | |
Screw L/D Ratio | 16.0:1.0 to 20.0:1.0 | ||
Screw Compression Ratio | 2.0:1.0 to 2.5:1.0 | ||
Vent Depth | 0.025 | mm |
Injection instructions |
---|
Santoprene TPV与乙缩醛和PVC不相容。更多关于加工和模具设计的信息,请查阅我们的《注射成型指南》。 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Melt Temperature | 191 - 224 | °C | |
Die Temperature | 191 - 224 | °C |
Extrusion instructions |
---|
Santoprene TPV与乙缩醛和PVC不相容。更多关于加工和模具设计的信息,请查阅我们的《挤出成型指南》。 |
Note Message | |
---|---|
1 . | C mould |
2 . | Method B, right-angle specimen (cut) |
3 . | Type 1 |
4 . | Type 1 |
5 . | Type a |
6 . | Type a |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
POLYLAC® PA-765B | CHI MEI CORPORATION | ABS | POLYLAC® |
TRILAC® ABS-EX1000 | Polymer Technology and Services, LLC | ABS | TRILAC® |
Delta IPP 2318 | Delta Polymers | PP Copolymer | Delta |
PELPRENE™ P50DFR | TOYOBO America, Inc. | TPEE | PELPRENE™ |
SHINSTRA AG35TKB (PA6) | Shinil Chemical Industry Co., Ltd. | Nylon 6 | SHINSTRA |