Category: | MDPE , Medium Density Polyethylene |
Manufacturer: | LyondellBasell Industries |
Trademark: | Lupolen |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 0HZgqR_Lupolen-4021-K-RM.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Lupolen 4021 K RM is a new generation hexene linear medium-density polyethylene for rotomolding. Typical customer applications include large tanks including agricultural and chemical storage containers and underground and infrastructure applications. Lupolen 4021 K RM is a fully UV-stabilized and pelletized polymer. Tests have shown that this material is resisting against the harmful effect of biodiesel fuel.** It is not intended for use in medical and pharmaceutical applications. ** Resistance is based on our latest patented technology |
General Information | |
---|---|
Additive |
|
Features |
|
Uses |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.940 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 4.0 | g/10 min | ISO 1133 |
Environmental Stress-Cracking Resistance | > 1000 | hr | ASTM D1693B |
Full Notch Creep Test 1(50°C) | 2.1 | day | ISO 16770 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 750 | MPa | ISO 527-2 |
Tensile Stress (Yield) | 19.0 | MPa | ISO 527-2 |
Tensile Strain (Yield) | 9.0 | % | ISO 527-2 |
Films | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Elongation (Break) | > 450 | % | ISO 527-3 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Impact Strength | ISO 8256/1A | ||
-30°C | 120 | kJ/m² | ISO 8256/1A |
23°C | 265 | kJ/m² | ISO 8256/1A |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Vicat Softening Temperature | 114 | °C | ISO 306/A50 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Melt Temperature | 180 - 210 | °C |
Extrusion instructions |
---|
Processing: Recommended range for PIAT (Peak Internal Air Temperature) is 180 - 210 "C. PIAT should not exceed 225 °C. |
Note Message | |
---|---|
1 . | 6.0 MPa, 2% Arkopal N100 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Moplen EP500M | LyondellBasell Industries | PP Impact Copolymer | Moplen |
Garaflex™ E 4832 NAT UV-LCF | AlphaGary | TPE | Garaflex™ E |
EMERGE™ PC 8430-10 | Trinseo | PC | EMERGE™ |
Hapflex™ 560-6 | Hapco Inc. | TP, Unspecified | Hapflex™ |
KPOL-LDPE LD K-8/918 | KPOL Chem Co. | LDPE | KPOL-LDPE |