Category: | PP, Unspecified , Polypropylene |
Manufacturer: | Polykemi AB |
Trademark: | POLYfill |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 0Dnmh1_POLYfill-PP-HJ752-UV.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
PP/Elastomer Mineral reinforced |
General Information | |
---|---|
Filler / Reinforcement |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.980 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 25 | g/10 min | ISO 1133 |
Molding Shrinkage | ISO 294-4 | ||
Across Flow | 0.80 to 1.0 | % | |
Flow | 0.80 to 1.0 | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | 22.0 | MPa | ISO 527-2 |
Tensile Strain | ISO 527-2 | ||
Yield | 9.0 | % | |
Break | 170 | % | |
Flexural Modulus (23°C) | 1700 | MPa | ISO 178 |
Flexural Stress | 32.0 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | ||
-30°C | 5.0 | kJ/m² | |
23°C | 23 | kJ/m² | |
Charpy Unnotched Impact Strength | ISO 179 | ||
-20°C | No Break | ||
23°C | No Break |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature 1 | |||
0.45 MPa, Unannealed | 100 | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 57.0 | °C | ISO 75-2/A |
Vicat Softening Temperature | |||
-- | 130 | °C | ISO 306/A50 |
-- | 53.0 | °C | ISO 306/B50 |
CLTE - Flow | 5.5E-5 to 6.5E-5 | cm/cm/°C | Internal Method |
Note Message | |
---|---|
1 . | 120°C/hr |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 1307 UP | RTP Company | PPS | RTP |
Modified Plastics MN 6/6-FG 20 | Modified Plastics, Inc. | Nylon 66 | Modified Plastics |
ExxonMobil™ LLDPE LL 6100.17 | ExxonMobil Chemical | LLDPE | ExxonMobil™ LLDPE |
KOPA® KN333HI4BL | Kolon Plastics, Inc. | Nylon 66 | KOPA® |
OmniCarb™ PC/PBT 400IM2 | OMNI Plastics, LLC | PC+PBT | OmniCarb™ |