TechnoDur PBT 4 GF10 black (9992)

Category: PBT , Polybutylene Terephthalate
Manufacturer: TechnoCompound GmbH
Trademark: TechnoDur
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: 0AAohq_TechnoDur-PBT-4-GF10-black-9992-.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
PBT, injection moulding, 10% glass fibre, heat stabilized, excellent flow ability and strength, for outdoor applications
General Information
Filler / Reinforcement
  • Glass fiber reinforced material, 10% filler by weight
Additive
  • heat stabilizer
Features
  • High strength
  • High liquidity
  • Thermal Stability
Appearance
  • Black
Forms
  • Particle
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Density 1.38g/cm³ISO 1183
Melt Volume-Flow Rate (MVR) (250°C/2.16 kg)19.0cm³/10minISO 1133
MechanicalNominal ValueUnitTest Method
Tensile Modulus 4700MPaISO 527-2/1
Tensile Stress (Break)95.0MPaISO 527-2/5
Tensile Strain (Break)4.0%ISO 527-2/5
FlammabilityNominal ValueTest Method
Flame Rating (0.800 mm)HBUL 94
InjectionNominal ValueUnit
Drying Temperature 120 - 140°C
Drying Time 2.0 - 4.0hr
Suggested Max Moisture 0.020%
Rear Temperature 250 - 265°C
Middle Temperature 250 - 265°C
Front Temperature 250 - 265°C
Nozzle Temperature 260 - 270°C
Processing (Melt) Temp 260 - 270°C
Mold Temperature 75.0 - 100°C
Injection Pressure 60.0 - 100MPa
Injection Rate Fast
Holding Pressure 40.0 - 80.0MPa
Back Pressure 1.00 - 3.00MPa
Screw Speed 80rpm
Injection instructions
Residence Time: 5 to 10 min
Resin Grade Manufacturer Category Trademark
RTP 136 RTP Company PP, Unspecified RTP
DOW™ LLDPE GRSN-2070 NT The Dow Chemical Company LLDPE DOW™ LLDPE
Andur 9000-AP/Curene® 280 Anderson Development Company PUR-Ether/TDI Andur
GTPO™ 8101 S&E Specialty Polymers, LLC TPO (POE) GTPO™
Infino NH-1029 LOTTE ADVANCED MATERIALS CO., LTD. PC+ABS Infino